In this paper, the interactions between two parallel cracks are investigated experimentally and numerically. Finite element models have been established to obtain the stress intensity factors and stress distributions of the parallel cracks with different positions and sizes. Fatigue crack growth tests of 304 stainless steel specimens with the single crack and two parallel cracks have been conducted to confirm the numerical results. The numerical analysis results indicate that the interactions between the two parallel cracks have an enhancement or shielding effect on the stress intensity factors, depending on the relative positions of the cracks. The criterion diagram to determine the enhancement or shielding effect between two parallel cracks is obtained. The changes of the stress fields around the cracks have been studied to explain the mechanism of crack interactions.
In this paper, the fatigue crack growth behavior of the base metal (BM), the weld metal (WM) and the heat-affected zone (HAZ) in the metal-inert gas (MIG) welded joints of the 06Cr19Ni10 stainless steel are analyzed and studied. Results of the fatigue crack propagation tests show that a new fatigue crack initiates at the crack tip of a pre-existing crack, then propagates perpendicular to the direction of cyclic fatigue loads. This observation indicates that the original mixed-mode crack transforms into the mode I crack. The WM specimen has the largest fatigue crack growth rate, followed by the HAZ specimen and the BM specimen. To illustrate the differences in fatigue crack growth behavior of the three different types of specimens, metallographic structure, fracture morphology and residual stresses of the BM, HAZ and WM are investigated and discussed. The metallographic observations indicate that the mean grain size of the HAZ is relatively larger than that of the BM. The fractographic analysis shows that the WM has the largest fatigue striation width, followed by the HAZ and the BM. It is also found that the depth of dimple in the WM is relatively shallower than the one in the HAZ and BM, implying the poor plasticity behavior of the material. Analysis results of the residual stress analysis demonstrate a high level of tensile residual stress appearance in the WM and HAZ.
11 August 2016 in International Journal of Materials Research
In this work, mixed mode fatigue crack propagation in the welding zone of 06Cr19Ni10 austenitic stainless steel was experimentally investigated. The effects of strain strengthening on crack growth paths and growth rates were studied. The experimental results demonstrated that a new crack initiated from the notch-crack tip and propagated in the direction perpendicular to the loading direction, suggesting a change of the crack mode from mixed mode to Mode I. Strain strengthening has no effect on the crack growth paths, while it does have some effect on the crack growth rates. The metallographic results indicate that the fraction of transformed martensite increases with strain-strengthening level. Finite element analysis results reveal that strain strengthening can significantly change the distribution of the residual welding stress.