We propose a new principle of adaptive Severe Plastic Deformation (SPD) processes, in which contact pressure stems from the reaction of the tool, rather than a force exerted on the workpiece externally. The reaction owes to special tool design utilizing a wedge effect. This approach ensures self-regulation of the deformation mode without the need for complex bidirectional loading systems. In addition, the equipment for adaptive processing can operate at loads which are substantially lower than those required for conventional SPD processing. Adaptability is analyzed by way of example for the High Pressure Sliding (HPS) process, for which theoretical justification, numerical calculations by the finite element method, and experimental verification are provided. It was established that, thanks to the self-regulation mechanism, the pressure is maintained automatically at the level necessary for plastic deformation of the workpiece. Experiments on copper samples showed the formation of an ultra-fine-grained structure. The results obtained demonstrate the efficacy of the adaptive HPS and open prospects for its application in the processing of thin-walled metal products.
The study presents the effect of hot deformation parameters on the structure and properties of Inconel 625 alloy. It was found that increasing the hot deformation temperature combined with impact loading allows for the production of a compact with low residual porosity and high mechanical properties. Based on the research results, the optimal conditions for the consolidation of the powder material were determined. It was noted that impact loading enables the formation of juvenile surfaces between particles, which enhances adhesion strength after hot deformation.
2 December 2023 in Physicochemical Mechanics of Materials
The structure, phase composition, basic mechanical and corrosion properties of powder aluminum matrix composites obtained by the hot forging (HF) were studied. The results of studies of the microstructure of synthesized master alloy of different composition revealed the presence of particles of the strengthening phase of different dispersion and shape, which are rather evenly distributed in the metal matrix. The method of X-ray phase analysis established the presence of titanium and aluminum carbide, and also a number of lines belonging to titanium aluminides Al3Ti, Al5Ti3, Al2Ti, AlTi3, Al5Ti2. Aluminium composite materials were strengthened by the Al–C–Ti master alloy of various composition. Studies of the samples obtained after HF showed that the microstructure of the composites is characterized by the presence of two phases: the basis is the aluminum matrix, in which the agglomerates of master alloy are distributed. The composites reinforced with 15 mass% of the master alloy (20Al–64Ti–16C) in the initial charge and obtained by the method of sintering and HF have increased strength characteristics and demonstrate absolute stability in a 3.5% NaCl solution, regardless of the phase composition of the master alloy.
The effect of various deformation schemes on the structure and properties of iron powder compacts was studied. Shear-intensive methods, such as high-pressure torsion and asymmetric rolling, provided anisotropic structures with minimal porosity and enhanced bonding. The highest green strength (420 MPa) was achieved using shear deformation, demonstrating its efficiency for powder densification.