The complex reaction between liquid solder alloys and solid substrates has been studied ex-situ in a few studies, utilizing creative setups to “freeze” the reactions at different stages during the reflow soldering process. However, full understanding of the dynamics of the process is difficult due to the lack of direct observation at micro- and nano-meter resolutions. In this study, high voltage transmission electron microscopy (HV-TEM) is employed to observe the morphological changes that occur in Cu6Sn5 between a Sn-3.0 wt%Ag-0.5 wt%Cu (SAC305) solder alloy and a Cu substrate in situ at temperatures above the solidus of the alloy. This enables the continuous surveillance of rapid grain boundary movements of Cu6Sn5 during soldering and increases the fundamental understanding of reaction mechanisms in solder solid/liquid interfaces.
21 November 2025 in Journal of Materials Science: Materials in Electronics
The present work investigates the influence of Indium (In) additions at 4, 8, and 12 wt.% on the microstructure, phase stability, anisotropic lattice behavior and mechanical performance of Sn-58Bi solder alloy. Alloys were fabricated via casting and characterized using differential scanning calorimetry (DSC), tensile testing, scanning electron microscopy with energy-dispersive X-ray spectroscopy (SEM/EDX), and synchrotron-based techniques including in situ X-ray diffraction (XRD) and micro-X-ray fluorescence (XRF). Indium addition progressively reduced the melting temperature from 142.52 °C (Sn-58Bi) to 116.33 °C (Sn-58Bi-12In), while broadening the pasty range. Microstructure analysis revealed the formation of BiIn intermetallic compounds and coarsened Bi-rich regions with increased In content. Synchrotron micro-XRF mapping confirmed the elemental segregation of Bi and In. In situ synchrotron XRD demonstrated that the BiIn phase is stable at room temperature but dissolves above 80 °C. Lattice parameter refinement of the rhombohedral Bi phase indicated anisotropic stabilization, with suppression of contraction along the a-axis upon In addition. Solderability assessment showed that Sn-58Bi-12In achieved the shortest wetting time of 1.356 s, and a thinner Cu6Sn5 intermetallic layer was observed at the solder/Cu interface. Mechanical testing revealed a tradeoff between strength and ductility where tensile strength decreased from 69 to 53 MPa, while elongation improved to 15.5% at 12 wt.% In. Fracture surface analysis indicated a transition from brittle to ductile failure with increasing In content. These results demonstrate that Indium addition effectively tailors the microstructural, thermal, and mechanical behavior of Sn-58Bi solder, making Sn-58Bi-xIn a promising candidate for low-temperature electronic packaging applications.
For reliable electronics, it is important to have an understanding of solder joint failure mechanisms. However, because of difficulties in real-time atomistic scale analysis during deformation, we still do not fully understand these mechanisms. Here, we report on the development of an innovative in situ method of observing the response of the microstructure to tensile strain at room temperature using high-voltage transmission electron microscopy (HV-TEM). This technique was used to observe events including dislocation formation and movement, grain boundary formation and separation, and crack initiation and propagation in a Sn-3 wt.%Ag-0.5 wt.%Cu (SAC305) alloy joint formed between copper substrates.
27 December 2024 in International Journal of Nanoelectronics and Materials (IJNeaM)
This study investigates the effects of multiple reflow cycles and isothermal aging on the shear strength and microstructure of SAC305/Sn58Bi/Cu-OSP hybrid solder joints. The joints combine SAC305 solder spheres and Sn58Bi solder paste reflowed on Cu-OSP substrates. Microstructural analysis revealed two distinct regions: a Bi-rich phase at the bottom and an Ag-rich phase at the top. Reflow cycles and isothermal aging at 85 °C, 125 °C, and 150 °C for up to 120 hours were evaluated for their impact on mechanical performance and reliability. Shear tests at 100 mm/s and 2000 mm/s showed that hybrid joints outperformed conventional SAC305/Cu-OSP joints, even after multiple reflow cycles. Aging at 85 °C and 125 °C had minimal impact on shear strength, indicating good stability under moderate conditions. However, aging at 150 °C, above the melting point of Sn58Bi (138 °C), caused a significant decrease in strength. These findings highlight the potential of hybrid solder joints for improved mechanical performance and thermal stability, offering advantages over conventional solder joints for advanced electronic packaging.
If electronics manufacturers and users are to have confidence in the reliability of the solder joints on which they rely, it is essential to have an understanding of the solder joint failure mechanisms and the role of dynamic recrystallisation in failure. However, due to difficulties in real-time atomistic scale analysis during deformation, we still do not fully understand these mechanisms. Here, we report the development of an innovative in-situ method using high voltage transmission electron microscopy (HV-TEM) for observation of the microstructural response of a solder joint to room temperature tensile loading. This technique was used to observe events including dislocation formation, dynamic recrystallisation, grain boundary separation, and crack formation and propagation in a Sn-3wt.%Ag-0.5wt.%Cu (SAC305) alloy joint formed between copper substrates.