Swift heavy ion (SHI) irradiation is an effective method for modulating the properties of thin oxide films by introducing defects, strains, and structural transformations. Here, we applied 516 MeV Xe31+ irradiation to BaTiO3 (BTO) thin films grown on Nb:SrTiO3 substrates to induce the generation of tracks and nanohillocks. Memristors with BTO films irradiated at a fluence of 5 × 1010 ions cm−2 displayed excellent retention and endurance characteristics. Moreover, the memristors exhibited highly stable synaptic plasticity functions such as excitatory/inhibitory post-synaptic currents (E/IPSC) and paired-pulse facilitation/depression (PPF/D). The memristors achieved a discrimination accuracy of 92.5% on given handwritten digit data by an artificial neural network with supervised learning. These results verify that the judicious application of SHI irradiation on thin oxide films is a viable strategy for exploring neuromorphic computation.
Neodymium-doped yttrium fluoride crystal has emerged as one of the most valuable functional materials, and has thus become a research hotspot and shown promising application value in recent years. In this work, utilizing 460 keV H and 6.0 MeV C ions implantation, the damage behavior, lattice structure change, spectral, and electrical characteristics of the Nd:YLF crystal induced by electronic and nuclear energy loss were investigated, utilizing complementary characterization techniques (X-ray diffraction, hardness and elastic (Young’s) modulus, micro-Raman, absorption, fluorescence spectra, and I–V characteristic curve). Thus, the annealing effect on the waveguide properties and the surface damage of the samples was discussed. The fabricated waveguide structure shows potential application in highly sensitive optoelectronic sensors.
Due to uncontrolled conductive filament (CF) formation and rupture during operation, CF randomness in SrTiO3-based memristors severely limits their stability and retention. To address this challenge, we employ swift heavy ion (SHI) irradiation—516 MeV Xe ions—on Pt/SrTiO3/Nb:SrTiO3 devices, introducing controlled ion track defects that guide filament formation. The irradiated memristors demonstrate remarkable performance improvements, achieving a lower SET voltage of 0.65 V (compared to 0.85 V for unirradiated devices), extended retention (>106 s vs <105 s), and superior stability (σ/μ = 0.06/0.06 vs 0.14/0.04). Moreover, these devices reliably emulate synaptic plasticity with minimal cycle-to-cycle variations (<7.2%), enabling high-fidelity neuromorphic applications. When deployed in simulated neural networks for handwritten digit recognition, the irradiated memristors attain a recognition accuracy of 91.6%, showcasing their robustness in real-time computing tasks. These results highlight SHI irradiation as an effective strategy to engineer defect-guided pathways in oxide memristors, advancing their applicability in stable, high-performance neuromorphic systems.
To optimize the design of silicon carbide (SiC) devices for applications in space and nuclear environments, this work introduces varying degrees of lattice damage into SiC through controlled irradiation conditions, with Raman spectroscopy revealing its damage evolution behavior and quantitatively characterizing the increasing trend of disorder with irradiation fluences. Fine analysis of the A1(LO) phonon mode demonstrates that proliferation of irradiation-induced acceptor centers and accumulation of scattering defects lead to significant attenuation of carrier concentration and mobility (cross-verified by Hall effect measurements), thereby causing degradation in electrical conductivity of SiC. Subsequent electrical testing confirms an orders-of-magnitude reduction in conductivity, establishing a quantitative correlation model with total disorder quantified by the DI/DS model. The non-destructive Raman technique enables simultaneous acquisition of material damage characteristics and quantitative electrical performance degradation, providing a predictive framework for the evolution of electrical behavior for SiC under irradiation damage, with significant implications for optimizing irradiation-hardened device designs.
In the high-energy mode of Booster Ring (BRing) of the High Intensity heavy-ion Accelerator Facility (HIAF), the pre-accelerated ions from the iLinac will be stripped by a carbon foil to higher charge states and then injected into the BRing. The thermal deposition and irradiation damage caused by high beam intensity and high energy deposition limit the lifetime of the foil. To ensure the stable operation of HIAF, a long-lifetime stripper foil with excellent irradiation and high-temperature resistance is required. This report aims to reveal the irradiation damage evolution of several kinds of carbon foils and its impact on their physical properties. Irradiation experiments were performed at HIRFL-SFC using Xe beams with the energy loss close to that of U beams in HIAF. There were three kinds of foils from four producer irradiated in the experiments, including Multilayer graphene (MLG) produced by KANEKA Co. and the Institute of Coal Chemistry (SXICC), diamond-like carbon (DLC) foil by the Institiute of Modern Physics (IMP) and Graphene Oxide (GO) foil by TIMESNANO Co. Various characterization methods were used to study the changes in surface morphologies, microstructures, and physical properties of the foils. The results indicated that MLG has a tendency for amorphization, DLC has a tendency for graphitization, and the oxygen-containing functional groups on the GO surface are damaged. These structural changes are expected to significantly impact the mechanical properties of the foils.