The paper describes the influence of the drum system construction of two modern carding machines on the porous structure of spunlace non-wovens composed of polyester and viscose. The non-woven fabric structure, including the number and size of the pores, determines the tensile strength of the composites obtained. The spunlace non-wovens were subjected to tensile strength tests in the machine, and cross-directions and microscopic observations of their structure were made. The results of the experiments were used to determine the relationship between the strength of the material and the porosity of its structure. This knowledge was used to prepare recommendations for the manufacturer of wet wipes in order to enable the selection of a carding machine for the mass production of final products with strength properties that meet market requirements and satisfy the end customer.
1 March 2022 in The Journal of the Textile Institute
This article presents an analysis of the images of the fibres produced in Spunlace technology, using two different types of modern cards, i.e. using a single card, then using the other card, singly, and finally, using the two cards in parallel. The fibre images were analysed for the presence and orientation of free spaces between carded and water-spiked fibres of viscose and polyester. The longitudinal and transverse strength of the fibres produced, was tested. On this basis, the correlations between the construction of the cards, the method of mixing the fibres and the strength of the non-woven fabric were determined. The research presented in the article could prove to be a useful source of information for carding machine manufacturers; moreover, it could be used by carder users, in order to improve the textile production process.
1 December 2024 in Advances in Science and Technology Research Journal
The article presents the results of experimental studies on selected, mechanical properties of three-layer film, produced by blown film extrusion. Three-layer film was developed for making garbage bags. The research was carried out under industrial conditions. The three-layer film sleeves tested...
The paper describes the influence of the drum system construction of two modern carding machines on the porous structure of spunlace non-wovens composed of polyester and viscose. The non-woven fabric structure, including the number and size of the pores, determines the tensile strength of the composites obtained. The spunlace non-wovens were subjected to tensile strength tests in the machine, and cross directions and microscopic observations of their structure were made. The results of the experiments were used to determine the relationship between the strength of the material and the porosity of its structure. This knowledge was used to prepare recommendations for the manufacturer of wet wipes in order to enable the selection of a carding machine for the mass production of final products with strength properties that meet market requirements and satisfy the end customer.
Viscose–polyester nonwovens are now widely used. The desired performance properties of these nonwovens, such as quality and strength, depend to a large extent on the carding process, in which homogenised layers of properly mixed fibres are formed. In this article, a comparative analysis of two different designs of modern, double-drum carders and their impact on the quality of fibre mixing and on the strength of the final nonwoven fabric is presented, based on research and tests carried out in an industrial production line. To this end, mathematical models were developed for the relevant indicators (fibre delay time and the average fibre circulation path length in the carding machine) that characterise the carding process. Based on numerical calculations, these indicators were determined for the actual geometry of the carding elements and the process parameters applied in the tests. A discussion is provided to interpret the values of these indicators and their correlation with the strength of the nonwoven fabric produced, taking into account the different design of the carders used in the tests. The results showed that the average fibre delay time ranged from 1.40 s to 1.99 s, while the corresponding fibre delay length varied between 4.42 m and 6.30 m. Moreover, the mean fibre circulation path length was greater in the second carding machine (20.5–26.4 m) than in the first (16.9–17.0 m), indicating more intensive longitudinal fibre mixing.
This study developed and implemented, under industrial conditions, a multi-criteria procedure for evaluating three-layer polyethylene films with a high regranulate content. A set of validated production formulations with varying secondary-material content was investigated. The methodology compared five mechanical properties with predefined, group-specific performance thresholds and used a non-compensatory Q index to express relative functional compliance; regranulate content was considered separately as an indicator of secondary-material use. Pareto front analysis was used to identify optimal material variants by considering the relationship between recycled content and their relative compliance with the applicable group-specific requirements. The proposed approach supports screening the functional properties of manufactured film products (high-strength refuse bags) at elevated recycled-material content levels.