SK5 steel is the base material used for the preparation of the wrinkle scraper, whose service life strongly affects the working efficiency and economic benefits. In this work, WC–Cr3C2–Ni coating was deposited on the SK5 steel substrate by using High-velocity air fuel spray (HVAF) and Laser cladding (LC) processes respectively, named HVAF-WC coating and LC-WC coating. The microstructure and wear resistance of both coatings were analyzed, and were compared with the substrate sample. Results showed that the coatings were adhesive well onto the substrate. More WC with fine crystals is retained in HVAF-WC coating due to low flame flow temperature, while WC of LC-WC coating is characterized by columnar crystals. The wear rate of HVAF-WC and LC-WC coating was 4.00 × 10−7 mm3/(N•m) and 3.47 × 10−6 mm3/(N•m), respectively, which was two and one orders of magnitude lower than SK5 steel with 3.54 × 10−5 mm3/Nm. HVAF-WC coating exhibited the best wear resistance because of significant fine grain strengthening, which wear mechanism is mainly dominated by abrasive wear. Thus, it was thought that HVAF-WC coating is more effective ways to improve the wear resistance of SK5 steel, comparing with LC-WC coating.
To decrease energy consumption and improve the performance of micro-arc oxidation (MAO) films on 6063 Al alloy, a policy of K2TiF6 additive and electrolyte temperature control was adapted. The specific energy consumption relied on the K2TiF6 additive and more particularly on the electrolyte temperatures. Scanning electron microscopy demonstrates that electrolytes with 5 g/L K2TiF6 can effectively seal the surface pores and increase the thickness of the compact inner layer. Spectral analysis shows that the surface oxide coating consists of γ-Al2O3 phase. Following 336 h of the total immersion process, the impedance modulus of the oxidation film, prepared at 25 °C (Ti5-25), remained 1.08 × 106 Ω·cm2. Moreover, Ti5-25 has the best performance/energy-consumption ratio with a compact inner layer (2.5 ± 0.3 μm). This research found that the time of the big arc stage increased with the temperature, resulting in producing more internal defects in the film. In this work, we employ a dual-track strategy of additive and temperature providing an avenue to reduce the energy consumption of MAO on alloys.
25 June 2026 in Journal of Colloid and Interface Science
Multi-axial forging (MAF) and aging were employed to process a high-strength aluminum alloy. The tensile properties, microstructure, and corrosion behavior were researched. After MAF, the strength of the alloy was observably increased, but the elongation was decreased. The strengthening mechanism resulted from dislocation multiplication and grain size reduction. After aging, strength was enhanced further, and elongation was improved. The strength and elongation are 561 MPa and 12.3%. Moreover, the corrosion resistance was obviously enhanced. The further strengthening is mainly attributed to the precipitation strengthening. The larger size and discontinuous distribution of grain boundary precipitates resulted in the alloy having higher corrosion resistance.