This paper presents the results of a study on the atomisation process of 316L material. The primary objective of the study was to obtain the highest quality, quantity and yield of 316L metal powder for the established atomisation parameters (torch current and wire feed speed) at the assumed process time. Using experiment planning according to the Taguchi method, 16 pairs of controllable variable parameters were developed. It was observed that the low current high-wire speed configuration resulted in the formation of a considerable amount of molten metal on the sonotrode platform. This phenomenon prevented the ultrasound system from working properly, so some of the processes were interrupted. The results obtained from the tests showed that torch current and wire feed speed are parameters that have a significant impact on the efficiency of the ultrasonic atomisation process. The highest efficiency was achieved by the process with a torch current of 100 A and a wire feed speed of 9 mm/s.
The aim of this study was to evaluate structural changes and their impact on the functional properties of Ti-6Al-4V and Ti-6Al-7Nb titanium alloys produced by L-PBF. In the as-built condition, these alloys, despite high strength due to the presence of metastable α’ martensite, exhibit limited ductility. The samples were subjected to heat treatment at 850–1000 °C for 1 h, followed by aging at 500 °C for 4 h in an argon atmosphere. Analysis revealed a gradual microstructural transformation from the columnar structure characteristic of L-PBF to an equilibrium Widmanstätten microstructure. As a result of the decomposition of martensite and the formation of an α + β phase mixture, changes in microhardness and mechanical properties were observed. After heat treatment, the microhardness decreased by 15% for Ti-6Al-4V (from 427 ± 1 HV to 362 ± 25 HV) and by 12% for Ti-6Al-7Nb (from 408 ± 6 HV to 359 ± 15 HV). The Ti-6Al-7Nb alloy exhibited higher maximum elongation (7.7 ± 1.1%) than Ti-6Al-4V (4.8 ± 0.5%) due to a greater fraction of the β phase. The results highlight the critical role of the controlled α′→α + β transformation in tailoring the properties of titanium alloys and provide a basis for optimizing manufacturing processes for medical and aerospace components.