Ce-modified MnCo2O4 flower-like nanosheet electrodes were prepared on nickel foam by a hydrothermal-calcination route and sequentially optimized with respect to reaction time, nominal Ce content, and PVP addition. Comparative SEM, XRD, XPS, and N2-sorption analyses identify MnCo2O4-9 h-3%Ce-PVP as the optimized electrode, with an open hierarchical nanosheet network and a BET surface area of 210.0 m2 g−1. The direct XRD/XPS control comparison distinguishes Ce-associated lattice and surface-state changes from PVP-associated synthesis effects without treating either trend as proof of substitutional Ce occupancy or quantitatively established oxygen vacancies. Likewise, PVP is treated as a morphology-directing additive whose transient adsorption or bridging role remains a synthesis hypothesis rather than a directly verified molecular mechanism. The optimized positive electrode delivers 2008 F g−1 at 1 A g−1, retains 1227 F g−1 at 20 A g−1, and shows 99.0% capacitance retention after 10,000 cycles at 5 A g−1. A carbon-supported iron oxide negative electrode, designated C/Fe2O3 only as a sample label because its exact oxide phase was not independently resolved by XRD or Raman spectroscopy, provides 443 F g−1 at 1 A g−1. The resulting charge-balanced asymmetric device operates over 0–1.6 V and delivers 34.6 F g−1 at 1 A g−1, corresponding to 12.30 Wh kg−1 at 0.8 kW kg−1. At 10 A g−1, it retains 29.8 F g−1 and delivers 10.60 Wh kg−1 at 8.0 kW kg−1, equivalent to 86.1% capacitance retention over a tenfold increase in current density. All device-level gravimetric values are calculated using the total active mass of both electrodes.
Transition-metal oxide/layered double hydroxide (LDH) electrodes often suffer from insufficient utilization of active sites, sluggish electron/ion transport, and limited cycling stability at high rates. Here, La-doped ZnCo2O4/MnCo-LDH nanoflowers serve as the positive electrode and Ti-supported Sb-doped SnO2 (Ti/Sb-SnO2) serves as the negative electrode for constructing an asymmetric supercapacitor. A stepwise hydrothermal route, La-doping regulation, and ethylenediamine-assisted morphology control transform stacked nanosheets into open porous nanoflowers with a specific surface area of 382.5 m2 g−1, thereby exposing more electroactive sites and shortening OH− diffusion pathways. La3+-induced lattice distortion and defect-related oxygen species further tune the electronic structure and improve interfacial charge-transfer kinetics. The optimized La-ZnCo2O4/MnCo-LDH electrode delivers 2130 F g−1 at 1 A g−1 and retains 1993 F g−1 after 10,000 cycles at 3 A g−1. The Ti/Sb-SnO2 negative electrode provides 673 F g−1 at 1 A g−1 and 302 F g−1 at 15 A g−1. The assembled device operates stably from 0 to 1.8 V in 2 M KOH and achieves 69 Wh kg−1 and 13,500 W kg−1.
A charge-balanced aqueous hybrid supercapacitor was constructed by coupling Co-modified MnWO4 nanorods with H2O2-treated carbon nanotubes (OH-CNTs) in 1 M KOH. The samples were designated by the nominal Co/(Mn + Co) precursor molar fraction; ICP-OES measured bulk Co fractions of 0.09 ± 0.01, 0.47 ± 0.03, and 0.75 ± 0.04 mol% for the nominal 0.1, 0.5, and 0.8 mol% samples, respectively. Rietveld refinement confirmed retention of the monoclinic P2/c MnWO4 phase with only small composition-dependent lattice changes. At an active-material loading of 2.00 ± 0.05 mg cm−2, the optimized nominal 0.5 mol% sample delivered 429.5 ± 11.0 C g−1 (119.3 ± 3.1 mAh g−1) at 1 A g−1 and retained 280.5 ± 8.5 C g−1 (77.9 ± 2.4 mAh g−1) at 15 A g−1. Because the positive electrode exhibits battery-type behavior, specific charge and specific capacity are used as the primary performance descriptors. Over −0.9–0 V vs. SCE, pristine CNT and OH-CNT electrodes delivered of 189.0 ± 7.2 and 246.6 ± 8.1 C g−1, corresponding to electrode-level apparent specific capacitances of 215 ± 8 and 280 ± 9 F g−1 at 1 A g−1 after correction for the measured IR drop. These values apply to the stated 90:5:5 CNT (or OH-CNT)/acetylene-black/PVDF formulation and CNT-active-mass normalization and should not be interpreted as intrinsic capacitances of isolated commercial MWCNT powders. Charge matching based on the measured gave m+/m− = 0.574; integration at the actual device loadings yielded q+ = 0.861 ± 0.015 C and q− = 0.854 ± 0.015 C (q+/q− = 1.008). The device operated over 0–1.6 V and delivered 97.9 ± 3.1 F g−1 at 0.51 A g−1, corresponding to 34.8 Wh kg−1 at 408 W kg−1 when normalized to the combined active mass of both electrodes. Three independently assembled devices retained 96.0 ± 0.7% of the initial capacitance and showed a coulombic efficiency of 98.8 ± 0.1% at the 10,000th cycle at 5.13 A g−1. Device metrics are normalized to the combined active mass of both electrodes and exclude current collectors, separator, electrolyte, and packaging.