At present, the packing method of “plastic bag–buffer packing–packing paper box” is adopted for bearing packaging. However, the common packing method has a poor packing effect and poor versatility. In this study, a new biomimetic cobweb cushion is proposed to solve the problem of insufficient cushioning capacity of high-precision bearing cushion packaging pads. First, according to the nature of cobweb form, the cobweb cushion structure configuration is determined. Next, based on the structure of the cushion and the relationship between the parameters of radial thread and spiral thread, a mechanical and target optimization model is established. The stress nephogram of bearing and the cobweb cushion are analyzed under three drop heights of 381, 610, and 700 mm, in the finite element simulation software to ensure that the maximum bearings stress is not beyond the material yield strength. Via the 3D printing technology, a cobweb cushion shell cast is made. Drop tests of the bearing were performed, and the results were verified with the finite element simulation analysis. This research can provide technical support for the protection of high-precision bearings from accidental drops during transportation.
Microbial fuel cells (MFCs) are promising bioelectrochemical systems for simultaneous wastewater treatment and energy recovery. However, their practical application is still limited by insufficient power output and weak transient energy-supply capability under fluctuating operational conditions. Herein, a bifunctional CF/MXene/FeS composite anode was fabricated through a one-step hydrothermal strategy to simultaneously enhance electricity generation and capacitive charge storage in MFCs. Unlike conventional bioanode modifications that primarily target conductivity enhancement alone, the constructed hierarchical composite integrates conductive MXene nanosheets and electroactive FeS phases to synergistically improve extracellular electron transfer and interfacial charge-storage behavior. The modified electrode exhibited enhanced surface roughness, abundant electroactive sites, and improved biofilm-supporting interfaces. Benefiting from the integrated conductive and electroactive composite framework, the CF/MXene/FeS anode achieved a maximum power density of 1.69 W/m2, which was 70.7% higher than that of pristine CF, together with an increased open-circuit voltage of 0.711 V. In addition, the composite electrode delivered a high total charge density of 13,192.09 C/m2 under the C900/D900 condition. Microbial community analysis further revealed substantial enrichment of electroactive bacteria, with the relative abundance of Geobacter increasing from 0.0058% to 22.84%. This work provides a promising strategy for integrating electricity generation and transient energy storage in bioelectrochemical systems, offering potential applications for energy-buffered MFCs under fluctuating power-demand conditions.
Transition-metal oxide/layered double hydroxide (LDH) electrodes often suffer from insufficient utilization of active sites, sluggish electron/ion transport, and limited cycling stability at high rates. Here, La-doped ZnCo2O4/MnCo-LDH nanoflowers serve as the positive electrode and Ti-supported Sb-doped SnO2 (Ti/Sb-SnO2) serves as the negative electrode for constructing an asymmetric supercapacitor. A stepwise hydrothermal route, La-doping regulation, and ethylenediamine-assisted morphology control transform stacked nanosheets into open porous nanoflowers with a specific surface area of 382.5 m2 g−1, thereby exposing more electroactive sites and shortening OH− diffusion pathways. La3+-induced lattice distortion and defect-related oxygen species further tune the electronic structure and improve interfacial charge-transfer kinetics. The optimized La-ZnCo2O4/MnCo-LDH electrode delivers 2130 F g−1 at 1 A g−1 and retains 1993 F g−1 after 10,000 cycles at 3 A g−1. The Ti/Sb-SnO2 negative electrode provides 673 F g−1 at 1 A g−1 and 302 F g−1 at 15 A g−1. The assembled device operates stably from 0 to 1.8 V in 2 M KOH and achieves 69 Wh kg−1 and 13,500 W kg−1.
A charge-balanced aqueous hybrid supercapacitor was constructed by coupling Co-modified MnWO4 nanorods with H2O2-treated carbon nanotubes (OH-CNTs) in 1 M KOH. The samples were designated by the nominal Co/(Mn + Co) precursor molar fraction; ICP-OES measured bulk Co fractions of 0.09 ± 0.01, 0.47 ± 0.03, and 0.75 ± 0.04 mol% for the nominal 0.1, 0.5, and 0.8 mol% samples, respectively. Rietveld refinement confirmed retention of the monoclinic P2/c MnWO4 phase with only small composition-dependent lattice changes. At an active-material loading of 2.00 ± 0.05 mg cm−2, the optimized nominal 0.5 mol% sample delivered 429.5 ± 11.0 C g−1 (119.3 ± 3.1 mAh g−1) at 1 A g−1 and retained 280.5 ± 8.5 C g−1 (77.9 ± 2.4 mAh g−1) at 15 A g−1. Because the positive electrode exhibits battery-type behavior, specific charge and specific capacity are used as the primary performance descriptors. Over −0.9–0 V vs. SCE, pristine CNT and OH-CNT electrodes delivered of 189.0 ± 7.2 and 246.6 ± 8.1 C g−1, corresponding to electrode-level apparent specific capacitances of 215 ± 8 and 280 ± 9 F g−1 at 1 A g−1 after correction for the measured IR drop. These values apply to the stated 90:5:5 CNT (or OH-CNT)/acetylene-black/PVDF formulation and CNT-active-mass normalization and should not be interpreted as intrinsic capacitances of isolated commercial MWCNT powders. Charge matching based on the measured gave m+/m− = 0.574; integration at the actual device loadings yielded q+ = 0.861 ± 0.015 C and q− = 0.854 ± 0.015 C (q+/q− = 1.008). The device operated over 0–1.6 V and delivered 97.9 ± 3.1 F g−1 at 0.51 A g−1, corresponding to 34.8 Wh kg−1 at 408 W kg−1 when normalized to the combined active mass of both electrodes. Three independently assembled devices retained 96.0 ± 0.7% of the initial capacitance and showed a coulombic efficiency of 98.8 ± 0.1% at the 10,000th cycle at 5.13 A g−1. Device metrics are normalized to the combined active mass of both electrodes and exclude current collectors, separator, electrolyte, and packaging.
To provide reliable input information for the load design and extraction of lunar soil water ice samples, it is necessary to study the water content distribution and water migration of simulated lunar soil water ice samples. On this basis, the temperature field model and the hydrothermal coupling relationship are proposed. The temperature field model was constructed by combining energy conservation and Fourier’s heat transfer law. The coupling relationship was established, and the hydrothermal coupling model was obtained by testing the unfrozen water content using the nuclear magnetic resonance method. Finite element software was used to solve the model numerically, and the water migration rule of the soil water ice samples at different ambient temperatures were analyzed. Thin-wall drilling tests were carried out on the simulated lunar soil water ice samples to obtain water content data for different locations, and the simulation results were verified. Due to the migration effect of the cold end of the water, the closer we tested to the edge of the sample, the higher the water content was. The higher the ambient temperature was, the more pronounced the water migration phenomenon of the whole sample was. These research results provide a basis for sampling scheme design.
The complex composition and extremely harsh, uncertain surface conditions on Mars impose stringent requirements on the coring performance and fault tolerance of a coring sampler. To satisfy the drilling and coring requirements of Martian soil–rock composite strata, a coring sampler capable of multiple repeated sampling operations is designed, which enables reliable acquisition and preservation of core samples. Drilling and coring experiments are conducted on simulated Martian soil with different particle size distributions and relative densities, as well as basalt specimens. The coring efficiency of the developed bit for Martian soil and rock under diverse working conditions, together with its wear characteristics during repeated coring, is systematically investigated. The results indicate that the proposed coring sampler structure is well adaptable to Martian soil–rock composite drilling. The coring mass of simulated Martian soil increases with increasing advance-to-rotation ratio and relative density, as well as decreasing median particle size. The coring mass of specimens with 91.7% relative density is significantly higher than that of 72.8%, and the maximum single coring mass of fine-grained pure regolith specimens reaches 19.32 g. During basalt coring, higher rotational speeds lead to more severe bit wear and more pronounced temperature elevation, with a peak temperature of 372.4 °C at 120 r/min. A rotational speed of 110 r/min achieves the best compromise between core integrity and bit service life, exhibiting excellent long-term operational stability and favorable cutting–rock-breaking matching performance. The results of this research provide a reference scheme and data support for future Martian soil–rock composite coring and drilling exploration missions.