This work investigates the structural evolution and electrocatalytic activity of the amorphous metal alloy Al87Y4Gd1Ni4Fe4 during short-term annealing and its effect on the kinetics of the hydrogen evolution reaction (HER) in 1 M KOH. It is shown that a 5 min heat treatment at 647 ± 2 K initiates controlled nanocrystallisation with the formation of AlFe2Ni, GdFe2 and Al(X) (X = Gd, Ni, Y, Fe) phases, which are uniformly dispersed in the amorphous matrix. According to XRD, DSC and HRTEM data, it was established that the formation of intermetallic nanodomains leads to a decrease in charge transfer energy barriers and the appearance of additional active centres of H* adsorption. Electrochemical studies have shown an increase in cathode current density, an increase in i0 by 2–3 orders of magnitude, and a decrease in Rct after annealing, confirming the improvement in HER kinetics. Potentiostatic tests showed an increase in the volumetric hydrogen evolution rate from 35.1 to 106.0 mL/(g·min) during the first immersion and up to 217.9 mL/(g·min) during reuse. SEM/EDS analysis revealed surface reconstruction and Ni enrichment after HER, which contributes to the acceleration of the H* recombination stage. The synergy of the amorphous matrix and nanophases ensures high electrocatalytic activity and stability of the system, making annealed AMA a promising low-cost catalyst for alkaline hydrogen evolution.
This study investigates the effect of short-term isothermal annealing at 647 ± 1 K for 5 min on the surface state, electrochemical response, and tribological behavior of the Al87Y4Gd1Ni4Fe4 amorphous alloy. Scanning Kelvin probe measurements revealed a pronounced shift in the contact potential difference and a more spatially coherent distribution of CPD after annealing, indicating substantial modification of the surface electronic state. XPS analysis showed that the relative contribution of oxidized Al increased from approximately 84.4% to 92.9%, whereas the contribution of non-oxide Al species decreased from approximately 15.6% to 7.1%. At the same time, the total surface oxygen concentration decreased and yttrium became enriched in the near-surface region, demonstrating a redistribution of surface chemical states rather than a simple increase in oxidation. Annealing caused only minor changes in surface roughness but markedly improved wear performance: the specific wear rate decreased from 1.917 × 10−3 to 1.234 × 10−3 mm3/(N·m) (approximately 36%), while the maximum wear-track depth decreased from 35.8 to 8.55 μm. In contrast, electrochemical impedance spectroscopy revealed deterioration of the protective properties of the surface layer. The passive-film resistance decreased from 7845 to 4335 Ω·cm2, the charge-transfer resistance from 8692 to 5262 Ω·cm2, and the double-layer CPE exponent ndl from 0.91 to 0.74, indicating increased electrochemical heterogeneity of the interface. Thus, short-term annealing produces a distinct functional trade-off: it substantially improves the tribological performance of the Al87Y4Gd1Ni4Fe4 alloy while simultaneously reducing the effectiveness of its electrochemical surface barrier.