27 December 2024 in Materials
Verified
Journal Article
Open access
PDF file
LZLei Zhao
Lei Zhao
YJYANG Jichun
YANG Jichun
FXFU Xiaoyang
FU Xiaoyang
The changes in the inclusions in 316L stainless steel before and after Ce addition were studied by adding different contents of Ce. The effects of rare earth Ce treatment on the modification of MnS inclusions in steel and the pitting corrosion resistance of 316L stainless steel are studied by field-emission scanning electron microscopy, laser confocal microscopy, the 6% FeCl3 corrosion weight loss test, and Tafel polarization curve test. The results show that the addition of Ce reduces the corrosion rate of stainless steel in 6% FeCl3 solution, and reduces the number and size of corrosion pits. The corrosion resistance is the best at a 0.0082% Ce content. In addition, the addition of Ce reduced the corrosion current density of stainless steel in 3.5% NaCl solution and increased the corrosion potential. The corrosion potential increased from −329 mV to −31.4 mV. Through Ce treatment, the grain is refined and the inclusions in the experimental steel are modified. With the increase in rare earth content, Mn S gradually transforms into Ce2O2 S inclusions. The morphology of the inclusions gradually change from the original long strips to a spherical shape, and the average size is significantly reduced, which improves the corrosion resistance of the stainless steel. The addition of rare earth Ce plays modifies the inclusions and purifies molten steel.

3 January 2020 in Metals
Verified
Journal Article
Open access
PDF file
FXFU Xiaoyang
FU Xiaoyang
BPBAI Pucun
BAI Pucun
YJYANG Jichun
YANG Jichun
The hot deformation of 18Cr-5Ni-4Cu nitrogen-alloyed austenitic stainless steel was tested with a Gleeble-1500D simulator in the temperature range of 1273–1473 K and in the strain rate range of 0.01–10 s−1. The Zener-Hollomon parameter method was used to construct a constitutive equation for high-temperature plastic deformation. The energy dissipation diagram of the material was calculated based on dynamic material modelling (DMM). The microstructural variations were characterized via X-ray diffraction (XRD), field emission scanning electron microscopy (FESEM) with energy dispersive spectroscopy (EDS) and transmission electron microscopy (TEM). The thermodynamic calculation results showed that the addition of nitrogen to 18Cr-5Ni-4Cu steel promoted the formation of Cr2N and gas phases and expanded the austenite phase region; these results were consistent with the XRD test results of the solid solution sample. The hot deformation activation energy after nitrogen addition was 556.46 kJ∙mol−1. The processing map predicted that the optimum hot working regimes were in the temperature range of 1416–1461 K, where ln ε ˙ was 0.75–1 on the power dissipation map. At high temperatures and a small strain rate, dynamic recrystallization easily occurred. The TEM analyses showed that nano-scale M23C6 and Cr2N precipitated at the grain boundary, and NbC with a diameter of approximately 150 nm appeared along the grain boundary, resulting in grain boundary strengthening. The phase precipitation results were consistent with the Thermo-Calc calculation results. The nitrogen solid solution in the steel promoted the precipitation of nitrides, which caused grain boundary strengthening. Thus, the grain boundary stress increased and wedge-shaped grain boundary cracks formed.

1 January 2024 in High Temperature Materials and Processes
Verified
Journal Article
Open access
PDF file
LZLei Zhao
Lei Zhao
JYJichun Yang
Jichun Yang
HHHongao Hu
Hongao Hu
FXFU Xiaoyang
FU Xiaoyang
Macroscopic and microscopic textures of non-oriented silicon steel hot rolled sheets with different rare-earth Ce contents were investigated using X-Ray Diffraction, Electron Back Scatter Diffraction, and field emission scanning electron microscopy, and the magnetic properties of the cold-rolled annealed sheets were examined using a silicon steel sheet testing system. The results show that the addition of rare-earth Ce reduces the proportion of unfavorable γ texture intensity and texture {111} and enhances the proportion of favorable η texture intensity and texture {100} and {110} in the steel. Magnetic property tests show that rare-earth Ce favors the reduction in test steel loss and the increase in magnetic susceptibility. The main reason is that rare-earth Ce combines with O and S in steel to form large-size inclusions, which preferentially precipitate in the liquid steel and inhibit the precipitation of fine AlN and MnS inclusions, while denaturing the inclusions to spherical composite inclusions such as Ce 2 O 2 S-MnS, CeS-AlN, and CeAlO 3 , thus exerting a good effect of purifying the liquid steel and denaturing the inclusions.

11 October 2018 in Metals
Verified
Journal Article
Open access
PDF file
FXFU Xiaoyang
FU Xiaoyang
BPBAI Pucun
BAI Pucun
YJYANG Jichun
YANG Jichun
The cracking initiation mechanism of high Cu-bearing nitrogen-alloyed austenitic stainless steel was systematically investigated by using a Gleeble-1500D simulator under different strains and deformation temperatures in the hot deformation process. The cracking initiation process and microstructure variations were characterized by optical microscopy (OM), X-ray diffraction (XRD), field emission scanning electron microscopy (FESEM) with energy dispersive spectroscopy (EDS) and transmission electron microscopy (TEM). In the deformation process, Cu-rich and Cr-rich phases were found around the microscopic crack at the strain of 0.5. Cu content was found to be higher at the grain boundary than inside the grain. The equilibrium phase diagram calculated by Thermo-calc shows that Cu precipitates out in the form of an elementary substance below 1022 °C, when the Cu mass fraction reaches 5%. Meanwhile, dislocation walls and twin crystals were observed by TEM. The results show that the synergistic effect of the secondary phases, such as M23C6 precipitated along the grain boundary and stress concentration, lead to crack generation, which is lower at high temperature and low temperature and is higher at 1100 °C and increase as the strain increases.