The effects of the solution heat treatment temperature on the precipitates, grain boundary evolution and response of the microhardness of Inconel 718 (IN718) superalloy fabricated by selective laser melting (SLM) were investigated. It was found that: (1) The long-chained Laves phases formed in the as-deposited condition dissolved into the matrix when the solution temperature rises above 980 °C. (2) The width-to-length ratio was maintained at approximately 1.6 when the solution was heated from 980 °C to 1080 °C, and dropped down to 1.03 when heated to 1130 °C. (3) Low-angle grain boundaries kept the same number fraction of 65% from 980 to 1080 °C as the as-deposited condition, and decreased dramatically from 1090 to 1130 °C to 4%. (4) Annealing twin boundaries occurred at 1090 °C with a number fraction of 3%, and quickly increased to 65% when heated to 1130 °C. It is concluded that the static recrystallization of IN718 fabricated by selective laser melting (SLM) occurred at 1090 °C and fast proceeded to full recrystallization at 1130 °C. The forming of annealing twins accompanies the recrystallization process and is an effective way to refine the recrystallized grain size.
Calcium silicate slag (CSS) is waste slag and it contains a large amount of beta-dicalcium silicate. This study is mainly focused on the effect of CSS on the hydration of cementitious pastes. CSS was used to partly replace cement, and composite pastes containing CSS and cement were prepared. The mineral composition and particle size distribution of CSS were characterized. The chemically combined water of the paste sample was measured at a given test age. Based on the value of chemically combined water, the hydration degree and the hydration rate of composite pastes were analyzed. The flexural strength of the samples was established. The pore structure and micromorphology of the sample were also observed. The results indicate the chemically combined water decreased, the hydration degree decreased, the hydration rate declined, and the spherical micromorphology of the calcium silicate hydrate gel was reduced after more cement was replaced by CSS in the composite pastes. Besides, the amount of pores increased, its size was bigger, and air content in the pore was higher. However, flexural strength was lower. CSS has a significant impact on the hydration of cementitious pastes, and it is thus suitable to regulate hydration.
The hot deformation of 18Cr-5Ni-4Cu nitrogen-alloyed austenitic stainless steel was tested with a Gleeble-1500D simulator in the temperature range of 1273–1473 K and in the strain rate range of 0.01–10 s−1. The Zener-Hollomon parameter method was used to construct a constitutive equation for high-temperature plastic deformation. The energy dissipation diagram of the material was calculated based on dynamic material modelling (DMM). The microstructural variations were characterized via X-ray diffraction (XRD), field emission scanning electron microscopy (FESEM) with energy dispersive spectroscopy (EDS) and transmission electron microscopy (TEM). The thermodynamic calculation results showed that the addition of nitrogen to 18Cr-5Ni-4Cu steel promoted the formation of Cr2N and gas phases and expanded the austenite phase region; these results were consistent with the XRD test results of the solid solution sample. The hot deformation activation energy after nitrogen addition was 556.46 kJ∙mol−1. The processing map predicted that the optimum hot working regimes were in the temperature range of 1416–1461 K, where was 0.75–1 on the power dissipation map. At high temperatures and a small strain rate, dynamic recrystallization easily occurred. The TEM analyses showed that nano-scale M23C6 and Cr2N precipitated at the grain boundary, and NbC with a diameter of approximately 150 nm appeared along the grain boundary, resulting in grain boundary strengthening. The phase precipitation results were consistent with the Thermo-Calc calculation results. The nitrogen solid solution in the steel promoted the precipitation of nitrides, which caused grain boundary strengthening. Thus, the grain boundary stress increased and wedge-shaped grain boundary cracks formed.