The rejuvenation behavior of an Zr50Cu40Al10 (at.%) metallic glass upon cryogenic cycling treatment has been investigated. At a high casting temperature, the microstructure of the glass is quite homogenous and thus, internal stress cannot be generated during cycling. Therefore, the glass cannot be rejuvenated by cryogenic cycling treatment. In the contrary, by lowering the casting temperature, nano-sized heterogeneity can be induced and subsequently generates the internal stress and rejuvenates the glass. Once the glass is rejuvenated, the more induced free volume can plasticize the glass with a higher plastic strain. These findings point out that the synthesis conditions can tailor the heterogeneity of the glass and subsequently affect the following rejuvenation behavior upon thermal treatment. It can also help understand the mechanisms of rejuvenation of metallic glass upon cryogenic cycling treatment.
Even though the Mg-based bulk metallic glasses (BMGs) have shown superior anti-corrosion properties compared with their crystalline counterparts, the brittleness of them limits the widespread application of these materials. In the present study, we have firstly introduced porous NiTi shape memory alloy particles into an Mg-Zn-Ca BMG by the direct adding method. This composite showed both improved compressive strength and corrosion resistance in Hank’s solutions than its monolithic glassy counterpart. The NiTi dispersoids among the matrix were likely to hinder the main shear band propagation, and also acted as the corrosion barriers. Furthermore, the porous nature of present added particle could further increase the interface areas, which should enhance the reinforcing effects compared with solid ones. This low-cost, high-anticorrosive composite was a good candidate as an engineering material.
1 October 2013 in Materials Science and Engineering: A
The Mg–Si alloys have low CTEs (coefficients of thermal expansion) and other merits, which contribute to their application potential in the electronic industry. However, the details of their thermal properties are still unclarified, and need more research. In this study, the thermal conductivities (TC) of Mg–xSi (x = 1 wt.%, 1.38 wt.%, 2 wt.%, 3 wt.%, and 4 wt.%) binary alloys and Mg–4Si–yCa (y = 0.2 wt.%, 0.4 wt.%, 0.6 wt.%, 0.8 wt.%, and 1.0 wt.%) alloys over the temperature range of 25–300 °C were systematically studied. The results show that the TC of Mg–xSi binary alloys decreases with the increase of Si content, while it increases slightly near the eutectic composition. The addition of a Ca element to Mg–4Si alloys has an obvious modification effect on the Mg2Si phase. When the Ca content increases constantly, the TC of the alloys decreases at first; then, there is a significant increase at the content of 0.8 wt.% Ca, and after that, it continues to decline. The mechanism is mainly related to the precipitation of the CaMgSi phase at 0.8 wt.% Ca content.