Effect of ultrasonic treatment (UT) on the microstructures and mechanical properties of Mg99.0-xNixY1.0 (x=0.5, 1.0, 1.5, at.%) alloys was investigated. With the increase of Ni content, the amount of eutectic structure, consisting of Mg, Mg2Ni phase and LPSO structure, increased while the mechanical properties decreased in as-cast alloys. After introducing UT to the melt, the secondary phases in these alloys were refined significantly and distributed uniformly, especially for long period stacking ordered (LPSO) structure. In Mg98.5Ni0.5Y1.0 alloy, the formation of MgNi4Y phase, which was distributed adjacent to the LPSO structure at the grain boundaries, was stimulated by UT. In Mg97.5Ni1.5Y1.0 alloy with UT, not only the width of grain boundaries were reduced, but also both the width of LPSO structure and that of eutectic structure were reduced. The optimal mechanical properties were obtained in Mg98.5Ni0.5Y1.0 alloy, which exhibited 206MPa in ultimate tensile stress and 7.96% in elongation, respectively. After UT, these properties were enhanced to 231MPa and 14.56%, respectively. The other alloys' mechanical properties were also enhanced significantly by UT.
The rejuvenation behavior of an Zr50Cu40Al10 (at.%) metallic glass upon cryogenic cycling treatment has been investigated. At a high casting temperature, the microstructure of the glass is quite homogenous and thus, internal stress cannot be generated during cycling. Therefore, the glass cannot be rejuvenated by cryogenic cycling treatment. In the contrary, by lowering the casting temperature, nano-sized heterogeneity can be induced and subsequently generates the internal stress and rejuvenates the glass. Once the glass is rejuvenated, the more induced free volume can plasticize the glass with a higher plastic strain. These findings point out that the synthesis conditions can tailor the heterogeneity of the glass and subsequently affect the following rejuvenation behavior upon thermal treatment. It can also help understand the mechanisms of rejuvenation of metallic glass upon cryogenic cycling treatment.
Even though the Mg-based bulk metallic glasses (BMGs) have shown superior anti-corrosion properties compared with their crystalline counterparts, the brittleness of them limits the widespread application of these materials. In the present study, we have firstly introduced porous NiTi shape memory alloy particles into an Mg-Zn-Ca BMG by the direct adding method. This composite showed both improved compressive strength and corrosion resistance in Hank’s solutions than its monolithic glassy counterpart. The NiTi dispersoids among the matrix were likely to hinder the main shear band propagation, and also acted as the corrosion barriers. Furthermore, the porous nature of present added particle could further increase the interface areas, which should enhance the reinforcing effects compared with solid ones. This low-cost, high-anticorrosive composite was a good candidate as an engineering material.
The Mg–Si alloys have low CTEs (coefficients of thermal expansion) and other merits, which contribute to their application potential in the electronic industry. However, the details of their thermal properties are still unclarified, and need more research. In this study, the thermal conductivities (TC) of Mg–xSi (x = 1 wt.%, 1.38 wt.%, 2 wt.%, 3 wt.%, and 4 wt.%) binary alloys and Mg–4Si–yCa (y = 0.2 wt.%, 0.4 wt.%, 0.6 wt.%, 0.8 wt.%, and 1.0 wt.%) alloys over the temperature range of 25–300 °C were systematically studied. The results show that the TC of Mg–xSi binary alloys decreases with the increase of Si content, while it increases slightly near the eutectic composition. The addition of a Ca element to Mg–4Si alloys has an obvious modification effect on the Mg2Si phase. When the Ca content increases constantly, the TC of the alloys decreases at first; then, there is a significant increase at the content of 0.8 wt.% Ca, and after that, it continues to decline. The mechanism is mainly related to the precipitation of the CaMgSi phase at 0.8 wt.% Ca content.
In this paper, the refinement effect of Al-5Ti-0.2C refiner on Al-Zn-Mg-Cu alloys was first investigated, and then the effects of three forming processes, i.e., Gravity Casting (GC), Squeeze Casting (SC), and Squeeze Casting after Ultrasonic Treatment (UT-SC), on microstructure and properties of Al-Zn-Mg-Cu alloys were studied. The results show that the refining effect of Al-5Ti-0.2C refiner is obvious; first, the average grain size of the alloy decreases and then increases with the increase in Ti content from 0.15 wt.% to 0.3 wt.%. The optimal amount of added Al-5Ti-0.2C is 0.2 wt.% Ti content. The good refining effect is attributed to the formation of TiC particles and Al3Ti compounds by the refiner, which can all be the nucleus of solidification. The poor refining effect when the Ti content was more than 0.2 wt.% is due to the formation of coarse Al3Ti particles. The results of three forming processes that cast Al-Zn-Mg-Cu alloys under the addition of Al-5Ti-0.2C with 0.2 wt.% Ti content show that the mechanical properties under the UT-SC process are the best; the tensile strength in the as-cast state reaches 367 MPa, and the elongation is 3.84%. The effect of tiny TiC particles in the refiner on the microstructure and properties of Al-Zn-Mg-Cu alloys is also discussed.
The Zr element is one of the important grain refiners for 7xxx series Al-Zn-Mg-Cu alloys, but the effect of Zr content more than 0.15 wt.% needs to be deeply investigated under the action of ultrasonic vibration. In this study, the effects of Zr contents (0.1 to 0.25 wt.%) on microstructure and mechanical properties of Al-Zn-Mg-Cu alloy were studied. The results showed that Zr element could refine grains, but when the Zr content was greater than 0.15 wt.%, the grain size was not uniform, the number of second phase particles increased, and the segregation of components became more serious. It was found that after ultrasonic treatment, the grain-size inhomogeneity was greatly improved, and the Zr content could be added up to 0.2 wt.%. When the Zr content is equal or lower than 0.2 wt.%, ultrasonic treatment can effectively improve the mechanical properties of materials by refining grains and weakening segregation. However, when the Zr content is up to 0.25 wt.%, the effect is getting worse.