Ultrasonic vibration (UV) treatment has been successfully applied to improve the particles distribution of nano-sized SiC particles (SiCp) reinforced Al-5Cu alloy matrix composites which were prepared by combined processes of dry high energy ball milling and squeeze casting. When UV treatment is applied, the distribution of nano-sized SiCp has been greatly improved. After UV for 1 min, large particles aggregates are broken up into small aggregates due to effects of cavitation and the acoustic streaming. After UV for 5 min, all the particles aggregates are dispersed and the particles are uniformly distributed in the composites. Compared with the Al-5Cu matrix alloy, the ultimate tensile strength, yield strength and elongation of the 1 wt% nano-sized SiCp/Al-5Cu composites treated by UV for 5 min are 270 MPa, 173 MPa and 13.3%, which are increased by 7.6%, 6.8% and 29%, respectively. The improvements of mechanical properties after UV are attributed to the uniform distribution of nano particles, grain refinement of aluminum matrix alloy and reduction of porosity in the composites.
6 June 2023 in Journal of Materials Research and Technology
The rejuvenation behavior of an Zr50Cu40Al10 (at.%) metallic glass upon cryogenic cycling treatment has been investigated. At a high casting temperature, the microstructure of the glass is quite homogenous and thus, internal stress cannot be generated during cycling. Therefore, the glass cannot be rejuvenated by cryogenic cycling treatment. In the contrary, by lowering the casting temperature, nano-sized heterogeneity can be induced and subsequently generates the internal stress and rejuvenates the glass. Once the glass is rejuvenated, the more induced free volume can plasticize the glass with a higher plastic strain. These findings point out that the synthesis conditions can tailor the heterogeneity of the glass and subsequently affect the following rejuvenation behavior upon thermal treatment. It can also help understand the mechanisms of rejuvenation of metallic glass upon cryogenic cycling treatment.
Nano-ceramic particles are generally difficult to add into molten metal because of poor wettability. Nano-SiC particles reinforced A356 aluminum alloy composites were prepared by a new complex process, i.e., a molten-metal process combined with high energy ball milling and ultrasonic vibration methods. The nano particles were β-SiCp with an average diameter of 40 nm, and pre-oxidized at about 850 °C to form an oxide layer with a thickness of approximately 3 nm. The mm-sized composite granules containing nano-SiCp were firstly produced by milling the mixture of oxidized nano-SiCp and pure Al powders, and then were remelted in the matrix-metal melt with mechanical stirring and treated by ultrasonic vibration to prepare the composite. SEM analysis results show that the nano-SiC particles are distributed uniformly in the matrix and no serious agglomeration is observed. The tensile strength and elongation of the composite with 2wt.% nano-SiCp in as-cast state are 226 MPa and 5.5%, improved by 20% and 44%, respectively, compared with the A356 alloy.
Nano-SiCp reinforced A356 aluminium alloy composites were prepared by solid–liquid mixed casting. Nano-SiC particles 40 nm in diameter were pre-oxidised at 850°C. Millimetre-sized composite granules were then fabricated by milling a mixture of nano-SiCp and Al powders, and then remelting to form an alloy melt, which was treated by mechanical stirring and ultrasonic vibration to prepare the composites. Results showed that nano-SiC particles were dispersed pretty well within the matrix and no serious agglomeration was observed. As the weight fraction of SiCp increased, the tensile strength, yield strength and elongation of the composites increased as well, by 22%, 62% and 24%, respectively, when compared to A356 alloy with 2wt-% nano-SiCp.