The effects of different surface pretreatments on the microtensile bond strength (µTBS) between a bulk-fill resin-based composite cavity base material (Bulk Base HARD II) and 4-META/MMA-TBB resin (Super-Bond EX), which is often used as a luting agent for indirect dental restorations, were investigated. Six experimental treatments were established: 10% citric acid/3% ferric chloride conditioner (10-3), self-etching primer (Teeth Primer; TP), silane coupling agent (M&C Primer; MC), 10-3+MC, TP+MC, and a control group with no treatment. The µTBS was measured after 1 week (immediate group) and 6 months (aged group) of water storage. There were no significant differences in µTBS among the immediate subgroups. However, the aged 10-3+MC group exhibited the highest bond strength, significantly outperforming the control group. On the other hand, the µTBS of the aged TP group was significantly lower than those of both aged 10-3 and 10-3+MC. MC alone did not enhance bond strength, and its application after TP led to a nonuniform surface morphology, raising concerns about adhesive stability. Failure mode analysis indicated that cohesive failure within the luting cement was predominant, with mixed failures being more frequent in the aged TP group. Overall, MC may not be necessary, and 10-3 conditioning does not adversely affect bond strength. Based on the results of this in vitro study, the most effective clinical practice entails pretreatment of the prepared cavity employing a citric acid/ferric chloride conditioner.
This study investigated the influence of solvent evaporation on the ultimate tensile strength (UTS) and water-related weight changes in contemporary universal dental adhesives. Two two-step universal adhesives (OptiBond eXTRa Universal and G2-BOND Universal) and two one-step universal adhesives (OptiBond Universal and BeautiBond Xtreme) were evaluated. Adhesives were used either under normal storage conditions or after active solvent evaporation by removal of the bottle caps and storage at 37 °C for 2 weeks. Hourglass-shaped specimens were prepared, light-cured, and stored in water at 37 °C for 1 h or 7 days prior to UTS testing (n = 10). Specimen weights were measured before and after water storage. For OptiBond eXTRa Universal, no significant difference in UTS was observed between the original and desiccated groups after 7 days of water storage (p > 0.05). In contrast, G2-Bond Universal exhibited significantly higher UTS values in the desiccated group compared with the original group (p < 0.05). In the original group, the one-step universal adhesives failed to polymerize under the original (non-evaporated) conditions, whereas adequate polymerization was achieved following active solvent evaporation. Weight changes after water storage varied depending on the adhesive composition. These results suggest that residual solvent may influence the polymerization behavior, mechanical performance, and water-related properties of universal dental adhesives, emphasizing the importance of adequate solvent evaporation before light curing.