Objectives.To compare the clinical performances of a self-adhering resin composite and a conventional flowable composite with a self-etch bonding system on permanent molars. The influence of using rubber dam versus cotton roll isolation was also investigated.Materials and Methods.Patients aged between 6 and 12 years and presenting at least two permanent molars in need of small class I restorations were selected. Thirty-four pairs of restorations were randomly placed by the same operator. Fifteen patients were treated under rubber dam and nineteen using cotton rolls isolation and saliva ejector. They were evaluated according to the modified USPHS criteria at baseline, 6 months, and 1 and 2 years by two independent evaluators.Results.All patients attended the two-year recall. For all measured variables, there was no significant difference between rubber dam and cotton after 2 years of restoration with Premise Flowable or Vertise Flow (value > 0.05). The percentage of restorations scored alpha decreased significantly over time with Premise Flowable and Vertise Flow for marginal adaptation and surface texture as well as marginal discoloration while it did not vary significantly for color matching. After 2 years, Vertise Flow showed a similar behaviour to the Premise Flowable used with a self-adhesive resin system.
The color stability of resin cements plays a key role in the achievement of esthetically-pleasant restorations. Resin luting materials can be mainly divided into two main classes: adhesive (relying on previous application of adhesive systems) or self-adhesive (also known as one-step cements). The different chemical compositions determine their physio-mechanical characteristics which, in turns, influence their color stability. To evaluate the color variations of different dual-cured resin cements after water aging, 80 disc-shaped specimens (15 mm in diameter and 1.2 mm thick) were obtained from the following resin cements (n = 10): (1) Maxcem Elite Universal, MCU (Kerr); (2) RelyX Universal, RXU (3M); (3) Calibra Ceram, CAL (Dentsply); (4) Multilink, MUL (Ivoclar-Vivadent); (5) Panavia V5, PAN (Kuraray); (6) Calibra Universal, CUN (Dentsply); (7) SpeedCEM Plus, SCP (Ivoclar); and (8) Panavia SA, PSA (Kuraray). After light-polymerization, the specimens were measured with a spectrophotometer and CIELab* values were recorded. The specimens were then placed in a digitally controlled thermostatic water bath at 60° for 30 days and afterwards the color measurements were repeated. Color differences were calculated for each specimen before and after water-aging procedures with ΔEab formula and the data were statistically analyzed (p < 0.05). The type of cement statistically influenced the ΔEab (p < 0.05), with MCU showing the lowest color variations (4.3 ± 0.7) whereas RXU and PSA the highest (16.9 ± 1.6 and 16.8 ± 1.2, respectively). No differences were observed between CAL, CUN and SCP (p = 0.05). Color stability is related to the chemical composition of the resinous luting materials, thus material dependent.
Objective: The aim of this in vitro study is to evaluate the effect of expiration date on some mechanical properties of resin composites after controlled storage of syringes and compules in a refrigerator at 4°C. Materials and Methods: Specimens were tested at 7 days after storage in distilled water at room temperature. The investigated properties are the static modulus of elasticity, the flexural strength, and the Vickers microhardness. Same batches of restorative materials were examined at baseline (at least 1 year before their expiration date) and 1 year after they expired. Results: Paired t-test is used to compare the results between the two groups using StatView software (version 5.0) SAS Campus Drive Cary, North Carolina, USA. Except for the flexural strength, no statistical differences were found between the mechanical properties of the expired and the unexpired group. Conclusion: The 1-year expiry date did not seem to affect the investigated mechanical properties.