Suining Zheng

Dr. Suining Zheng

Chang'an University, Xi'an, China
orcid

Research Focus & Metrics

Academic Career Length

4Years (2023-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
19 January 2024 in Construction and Building Materials
Verified
Journal Article
Closed access
Suining ZhengSuining Zheng
Suining Zheng
HCHuaxin Chen
Huaxin Chen
Yue XiaoYue Xiao
Yue Xiao
YLYimin Liu
Yimin Liu
DKDongliang Kuang
Dongliang Kuang
HQHeping Qiu
Heping Qiu

3 May 2026 in Polymers
Verified
Journal Article
Open access
PDF file
AXAnhua Xu
Anhua Xu
LWLaifa Wang
Laifa Wang
Suining ZhengSuining Zheng
Suining Zheng
JTJia Hui Ting
Jia Hui Ting
XWXinyan Wang
Xinyan Wang
HCHuaxin Chen
Huaxin Chen
Styrene butadiene rubber (SBR) is a commonly used polymer modifier that can improve the mechanical properties and durability of cement mortar. However, the effects of different emulsifier types on cement hydration behavior and structural evolution still need to be systematically studied. To clarify the differences among anionic, cationic, and nonionic SBR emulsions on mortar performance, three types of SBR emulsion were selected in this study. Setting time, chemically bound water, mechanical properties, chloride ion diffusion, freeze–thaw cycles, and microstructure were tested to evaluate the effects of different types and dosages on cement mortar. The results show that all three types of SBR emulsion prolong the setting time of cement paste and reduce the early hydration degree. The cationic SBR emulsion shows a more obvious effect. At 28 d, the compressive strength of mortar with 10% cationic SBR emulsion increases from 38.5 MPa to 41.2 MPa, and the flexural strength also increases. In terms of impermeability, the chloride ion diffusion coefficient decreases from 7.47 × 10−12 m2/s to 5.12 × 10−12 m2/s after adding 10% cationic SBR emulsion. After 100 freeze–thaw cycles, the compressive strength loss of ordinary mortar is 16%, while it decreases to 7.2% with 15% cationic SBR emulsion, and the mass loss is also reduced. Microstructural analysis shows that the modified mortar has a denser internal structure, improved interfacial continuity, and reduced crack development after freeze–thaw cycles.

10 June 2026 in Materials
Verified
Journal Article
Open access
PDF file
SWSiyu Wu
Siyu Wu
HCHuaxin Chen
Huaxin Chen
Suining ZhengSuining Zheng
Suining Zheng
YDYonglu Dong
Yonglu Dong
WZWen Zhang
Wen Zhang
To address the lack of systematic quantitative studies on waterborne epoxy resin (WER)-modified emulsified asphalt regarding its rheological optimization and engineering applicability, this study fills the gap by preparing WER-modified emulsified asphalt via a two-step process. New findings reveal that 20% WER content significantly enhances elastic components, creep–recovery, fatigue life, and fracture energy. The main objective is to establish a theoretical basis for high-performance pavement materials. Modified emulsified asphalt specimens with different waterborne epoxy resin contents were prepared using a two-step method of “emulsification followed by compounding”. The stability of the emulsions was quantitatively evaluated by zeta potential, storage stability, particle size distribution, and demulsification time. Their rheological parameters, multi-stress creep–recovery characteristics, fatigue life, and low-temperature crack resistance were systematically tested across the full temperature range using a dynamic shear rheometer and a bending beam rheometer. In addition, the bonding performance, strength development behavior, and water resistance durability were comprehensively assessed through pull-out tests, Marshall stability and splitting strength tests, as well as freeze–thaw cycle tests. These properties were compared with those of unmodified emulsified asphalt (UEA-0) and SBR-modified emulsified asphalt (SBR-EA). With an increase in waterborne epoxy resin content, the elastic component of the modified asphalt improved significantly, and the phase angle continuously decreased. The specimen with 20% waterborne epoxy resin content (WER-EA-20) exhibited the best performance: its phase angle was lower than those of the other groups under high-, medium-, and low-temperature conditions. After seven creep–recovery cycles, its creep–recovery rate remained at 33%, substantially higher than the 8% observed for the unmodified specimen. The fatigue life reached 15,000 cycles under a shear stress of 2.1 MPa. At −10 °C, the fracture strength was 0.92 MPa, and the fracture energy reached 21.4 J. Furthermore, the pull-out strength of WER-EA-20 was 0.86 MPa, with the failure mode identified as asphalt cohesive failure. After 37 days of curing, the Marshall stability reached 22.5 kN, and the splitting strength was 1.36 MPa. After 40 freeze–thaw cycles, the freeze–thaw splitting strength ratio (TSR) of WER-EA-20 remained above 75%, representing an improvement of more than 110% compared to the unmodified UEA-0 (TSR ≈ 35.5%), which highlights the significant enhancement in water resistance imparted by the waterborne epoxy resin. Compared to SBR-EA, WER-EA-20 has a higher softening point, a lower suitable mixing temperature, and better anti-aging properties. Waterborne epoxy resin can effectively improve the viscoelastic properties and overall road performance of emulsified asphalt, and the modification effect increases with increasing dosage.

28 July 2026 in International Journal of Concrete Structures and Materials
Verified
Journal Article
Open access
PDF file
MXMingliang Xing
Mingliang Xing
HCHaomin Chen
Haomin Chen
AXAnhua Xu
Anhua Xu
HCHuaxin Chen
Huaxin Chen
Suining ZhengSuining Zheng
Suining Zheng
Yao SunYao Sun
Yao Sun
Superabsorbent polymers (SAP) can absorb and subsequently release large amounts of water, with uptake reaching several hundred times their dry mass under a

18 May 2023 in Vibroengineering PROCEDIA
Verified
Journal Article
Open access
PDF file
MSMei Song
Mei Song
Suining ZhengSuining Zheng
Suining Zheng
HMHaichen Mi
Haichen Mi
PXPeng Xu
Peng Xu
CZChongshang Zhang
Chongshang Zhang
Matrix and SBS modified asphalt mortar were prepared by replacing mineral powder with cement under different filler-asphalt ratios. The variation laws of ductility, softening point, penetration, cone penetration, and Brookfield rotational viscosity of the two kinds of pastes with filler-asphalt ratio were studied. The shear strength of the two kinds of asphalt mortar was calculated. And the viscosity-temperature curve was established. The best filler-asphalt ratio was recommended. The results show that the addition of cement and the increase of filler-asphalt ratio will reduce the ductility, penetration, and cone penetration of asphalt mortar, while improve the softening point, shear strength, and viscosity. In a specific range of filler-asphalt ratios, cement can improve the high-temperature performance of asphalt mortar without significant impact on the low-temperature performance.

28 July 2026 in Polymers
Verified
Journal Article
Open access
PDF file
Suining ZhengSuining Zheng
Suining Zheng
JXJiming Xiao
Jiming Xiao
HCHuaxin Chen
Huaxin Chen
AXAnhua Xu
Anhua Xu
RWRuiyang Wang
Ruiyang Wang
FLFulu Li
Fulu Li
Ethylene–vinyl acetate (EVA) as a redispersible polymer can improve the workability, mechanical properties, and interfacial bonding of repair mortar, but the regulatory effect of different EVA dosages on underwater performance remains unclear. This study investigates EVA–polyacrylamide (PAM) composite-modified repair mortar and systematically evaluates the influence of varying EVA content on mortar performance. Multi-scale methods including setting time measurement, flowability test, flexural and compressive strength tests, underwater flexural bonding strength, water-to-air strength ratio, cement loss rate, porosity, and scanning electron microscopy (SEM) characterization were employed. The results indicate that mortar with 8% EVA exhibits the optimal overall performance. The initial setting time of the cement paste increased from 35 to 47 min, and the final setting time from 55 to 72 min, improving workability. In terms of mechanical properties, the 28-day flexural strength increased from 7.5 to 9.2 MPa, and the compressive strength from 44.4 to 50.6 MPa. Regarding underwater performance, the 28-day underwater flexural bonding strength rose from 5.1 to 6.5 MPa; the water-to-air strength ratio increased from 79.1% to 95.2%, and cement loss rate decreased from 3.18% to 0.32%; pH changes were maintained within a moderate range. Microstructural analysis shows that the total porosity at 28 d decreased from 16.8% to 13.5% for mortar containing 8% EVA, and SEM observations revealed that hydration products uniformly filled pores forming a dense network, consistent with the trends of mechanical and interfacial bonding performance enhancement.