Gadolinium oxide (Gd2O3) nanoparticles were prepared via the reaction of gadolinium nitrate hexahydrate (Gd (NO3)3·6H2O) and ethylamine (C2H5NH2), and their surface morphology, particle size, and properties were examined by using scanning electron microscopy, X-ray diffraction (XRD), Raman spectroscopy, Fourier transform infrared (FT-IR) spectroscopy, and ultraviolet visible (UV-vis) spectroscopy. The Gd2O3 nanoparticles were used as the photocatalyst for the degradation of various azo dyes, such as methyl orange (MO), acid orange 7 (AO7), and acid yellow 23 (AY23) under irradiation with UV light. The effect of the experimental parameters (initial concentration of azo dyes, dosage of catalyst, and wavelength of UV light) on the photocatalytic properties of the Gd2O3 nanoparticles were investigated. At a constant H2O2 concentration, the photocatalytic degradation efficiency of the Gd2O3 nanoparticles for various azo dyes was in the order: methyl orange > acid orange 7 > acid yellow 23. The kinetics study showed that the photocatalytic degradation of azo dyes was followed by a pseudo first-order reaction rate law.
1 January 2015 in Nanomaterials and Nanotechnology
A gold nanoparticle solution was prepared by adding sodium borohydride (NaBH4), trisodium citrate dihydrate (C6H5Na3O7·2H2O), cetyltrimethyl ammonium bromide (CTAB,(C16H33)N(CH3)3Br), ascorbic acid (C6H8O6), and potassium tetrachloroaurate(III)(KAuCl4) to distilled water and stirring the solution for 15 min. [C60]fullerene nanowhisker-gold nanoparticle composites were synthesized using C60-saturated toluene, the gold nanoparticle solution, and isopropyl alcohol by liquid-liquid interfacial precipitation (LLIP). The product of the nanocomposites was characterized by X-ray diffraction, scanning electron microscopy, Raman spectroscopy, transmission electron microscopy, and solid-state 13C-nuclear magnetic resonance spectroscopy. The catalytic activity of the [C60]fullerene nanowhisker-gold nanoparticle composites was confirmed in 4-nitrophenol reduction by UV-vis spectroscopy.
Under ultrasonication, cycloaddition of [70]fullerene with various 2‐azidoethyl per‐O‐acetyl glycopyranoside of D‐mannose, D‐galactose, D‐glucose, D‐xylose and D‐maltose yielded glycosyl [70]fullerene derivatives 2a–2e. Based upon 1H‐ and 13C‐NMR, FT‐IR, UV‐vis, and FAB‐MS analyses, 2a–2c and 2e were a mixture of the major closed [5,6]‐bridged isomer product and two isomers as the minor, monoaddition products. However, in the case of D‐xylose, 2d was an unusual mixture of four mono‐adducts in the ratio of ca. 9:11:10:4.
In this study, a phosphorous-containing polyol (P-polyol) was synthesized and reacted with isophorone diisocyanate (IPDI) to produce water-dispersed polyurethane. To synthesize waterborne polyurethanes (WPUs), mixtures of P-polyol and polycarbonate diol (PCD) were reacted with IPDI, followed by the addition of dimethylol propionic acid, to confer hydrophilicity to the produced polyurethane. An excess amount of water was used to disperse polyurethane in water, and the terminal isocyanate groups of the resulting WPUs were capped with ethylene diamine. P-polyol:PCD molar ratios of 0.1:0.9, 0.2:0.8, and 0.3:0.7 were used to synthesize WPUs. The films prepared by casting and drying the synthesized WPUs in plastic Petri dishes were used to test the changes in physical properties induced by changing the P-polyol:PCD molar ratio. The experimental results revealed that the tensile strength of PU-10, the WPU with a P-polyol:PCD molar ratio of 0.1:0.9, was 16% higher than that of the reference P-polyol–free WPU sample. Moreover, the thermal decomposition temperature of PU-10 was 27 °C higher than that of the reference sample.