The hydrogen permeation behavior of novel AlCrFeTiNb, AlCrMoNbZr and AlCrFeMoTi high-entropy alloy (HEA) coatings were investigated. The hydrogen permeability of HEA coatings prepared by magnetron sputtering technology were tested using gas-driven deuterium permeation and electrochemical hydrogen permeation methods. The gas-driven permeation results show that the deuterium permeation resistance of the AlCrFeTiNb coating is the worst because of the unstable structure at a high temperature. Scanning electron microscope (SEM) and X-ray Diffraction (XRD) analysis proved a loose surface morphology of the AlCrFeTiNb coating and demonstrated the formation of iron-based oxides after deuterium permeation experiments. A high content of iron in HEA coating is disadvantageous for improving the hydrogen permeability. Differently, electrochemical hydrogen permeation reveals that the AlCrMoNbZr coating could resist hydrogen permeation better in a corrosive environment (0.2 mol/L KOH solution). The AlCrFeMoTi coating was peeled off after an electrochemical hydrogen permeation test due to the poor corrosion resistance. The hydrogen behavior of HEA coatings was discussed in detail. Our study provides a promising thought on hydrogen permeation of HEA coatings.
In a tritium-breeding blanket of a fusion reaction, helium, used as a tritium-purging gas, will purge the tritium breeder pebble beds to extract the tritium in blanket. The purge gas flow characteristics will affect the tritium extraction efficiency. The effect of the fixed wall on the pebble packing structures and purge gas flow characteristics was investigated by combining the discrete element method (DEM) and computational fluid dynamics (CFD) method. The results indicate that the fixed wall leads to a regular packing of the pebbles adjacent to the fixed wall in association with drastic fluctuations in the porosity of the pebble bed, which can affect the purge gas flow behaviors. Further analyses of helium flow behaviors show that the helium pressure in the pebble bed decreases in a linear manner along the flow direction, whereas the pressure drop gradient of helium increases gradually with an increase in the packing factor. The reduction in porosity in the pebble bed leads to a notable escalation in helium flow velocity. Concerning the direction perpendicular to the helium gas flow, the evolution of the cut-plane averaged velocity of helium is similar to that of the porosity, except in the region immediately adjacent to the wall. The pressure drop and flow characteristics obtained in this study can serve as input for the thermohydraulic analysis of the tritium blowing systems in the tritium-breeding blanket of a fusion reactor.
The flow characteristics of purge gas helium in the pebble bed of the tritium breeding blanket are important in analyzing the tritium purging process and optimizing the design of the solid breeder blanket. Therefore, the flow characteristics of helium gas in randomly packed pebble beds are investigated experimentally with a focus on the analysis of the pressure loss distribution. The results show that gas velocity, bed dimension, and pebble diameters have an obvious influence on the helium flow characteristics in pebble beds. With the increase in the inlet helium gas velocity, the pressure drop gradient of helium in the pebble bed gradually increased. With increases in the pebble bed dimension, the pressure drop gradient of helium in the pebble bed gradually increased. With the increase in the pebble diameter, the pressure drop gradient gradually decreased. In addition, the effect of temperature on the pressure drop of helium in the pebble bed was also preliminarily investigated. The pressure drop gradient of the helium through the pebble bed obviously increased with the increase in the helium and the bed temperature. The experimentally obtained pressure loss characteristics can be used for the validation of the simulation of a blanket pebble bed and as input parameters in the thermo-hydraulic analysis of solid-tritium breeder blankets.
Lithium-containing ceramics were significant tritium breeders for the fusion blanket concept, for which tritium release performance and mechanical properties serve as the core indicators for evaluating their performance as tritium breeders. The Li4Si0.8Ti0.2O4 material was designed as an advanced tritium breeder and fabricated into ceramic pebbles via the freeze-drying method. The tritium release properties of the Li4Si0.8Ti0.2O4 sample pebbles were investigated via temperature-programmed desorption (TPD). The mechanical properties of the same batch of tritium breeder pebbles were analyzed comparatively, specifically examining the change in their compressive strength before and after irradiation. The sample pebbles irradiated with different neutron doses show different tritium release characteristics, and the tritium release temperature was about 293–553 °C. This was due to the H2-tritium isotope exchange reaction, and radiation with different neutron doses will lead to different release temperatures of tritium. The mechanical properties of the Li4Si0.8Ti0.2O4 ceramic pebbles decreased significantly after irradiation. The main reason was that the accumulation of lattice defects and helium bubbles produced by high-energy neutron irradiation leads to internal cracks and helium embrittlement in the material. These results indicate that Li4Si0.8Ti0.2O4 solid solution may be considered a potential candidate for tritium breeder materials.