A series of trials to fusion weld commercially pure titanium (CPTi) to stainless steel 304 (SS304) have been conducted using laser beam welding (LBW) and gas tungsten arc welding (GTAW). Neither technique produced adequate weld joints with LBW showing a more promising result, while GTAW yielded separation of the workpieces immediately after welding. Cracking and fracturing took place mainly on the SS304 side, which was explained by the differences in the materials’ thermal properties. Various intermetallic phases formed during welding that were identified using energy dispersive X-ray spectroscopy (EDS) and electron backscattered diffraction (EBSD) technique and were compared with an isothermal ternary phase diagram of Fe-Cr-Ti. Their corresponding hardness values are reported and correlated with alloy compositions.
11 April 2019 in Metals and Materials International
Ti-5Al-5V-5Mo-3Cr (Ti5553) is a metastable β titanium alloy with a high potential use in the aeronautic industry due to its high strength, excellent hardenability, fracture toughness and high fatigue resistance. However, recent research shows this alloy has a limited weldability. Different welding technologies have been applied in the literature to weld this alloy, such as electron beam welding (EBW), gas tungsten arc welding (GTAW) or laser beam welding (LBW) under keyhole regime. Thus, in tensile tests, joints normally break at the weld zones, the strength of the welds being always lower than that of the base metal. In the present work, a novel approach, based on the application of LBW under conduction regime (with a High-Power Diode Laser, HPDL), has been employed for the first time to weld this alloy. Microstructure, microhardness and strength of obtained welds were analyzed and reported in this paper. LBW under conduction regime (LBW-CR) leads to welds with slightly higher values of Ultimate Tensile Strength (UTS) than those previously obtained with other joining processes, probably due to the higher hardness of the fusion zone and to lower porosity of the weld.
Understanding how feed rate (ft) affects tool deterioration during milling of Ni-based superalloys is practically important, but this understanding is currently insufficient. In the present study using a 718Plus Ni-based alloy and cemented tungsten carbide tool inserts, milling experiments were conducted with ft = 0.10 mm/tooth under either dry or wet (with coolant) conditions. The results are compared to those based on using ft = 0.05 mm/tooth from previous studies. The milling force (F) was monitored, the cutting tool edge was examined and the flank wear (VBmax) was measured. As would be expected, an increase in ft increased F. It was found that F correlated well with VBmax for the high ft (0.1 mm/tooth) experiments, as opposed to the previously observed poor F-VBmax relationship for the lower ft (0.05 mm/tooth) value. This is explained, supported by detailed failure analysis of the cutting tool edges, by the deterioration mode to be dominantly edge chipping with a low occurrence of fracturing along the flank face when the high ft was used. This dominancy of the deterioration mode means that the tool edge and workpiece contact was consistent and thus resulted in a clear F-VBmax relationship. A clear F-VBmax relationship should then mean monitoring VBmax through monitoring F is possible.
Butt welded joins were produced between commercially pure titanium and various titanium alloys using an electron beam welding technique. The materials used represent commercially pure grade, α-β alloy and β alloy. They were CP Ti, Ti-6Al-4V (Ti64) and Ti-5Al-5V-5Mo-3Cr (Ti5553), respectively. Grains were largest in the FZs of the different weldments, decreasing in size towards the heat affected zones (HAZs) and base metals. Hardness measurements taken across the traverse cross-sections of the weldments were constant from base metal-to-weld-to-base metal for CP Ti/CP Ti and Ti64/Ti64 welds, while the FZ of Ti5553/Ti5553 had a lower hardness compared with the base metal. During tensile testing the CP Ti/CP Ti weldments fractured at the base metal, whereas both the Ti64/Ti64 and Ti5553/Ti5553 broke at the weld zones. Fracture surface analysis suggested microvoid coalescence as the failure mechanism. The compositional analysis showed a relatively uniform distribution of solute elements from base metal-to-weld-to-base metal. CP Ti has always been known for its excellent weldability, Ti64 has good weldability and, preliminary results indicated that Ti5553 alloy is also weldable.