The generation of high-brightness white light in laser-illuminated devices is achieved by exciting yellow-green phosphors with a blue laser source. This configuration offers advantages such as high energy density and strong central luminous intensity. Among luminescent materials, LuAG:Ce phosphor ceramics (PCs) are notable for their high thermal stability and luminous output. In this study, LuAG:Ce PCs were produced from co-precipitated monophase nanopowders. The effects of vacuum sintering and air annealing temperatures on their porosity and luminescent properties were investigated. The sample, sintered at 1550°C and subsequently annealed at 1350°C, exhibited 3.5 vol.% porosity, highest room-temperature emission intensity in the series, and retained 96% of that intensity upon heating to 250°C. Under 450 nm laser-diode excitation, the sample achieved a luminous efficacy of 229 lm·W$^{-1}$ while maintaining excellent thermal stability. These results indicate that introducing controlled porosity to act as light-scattering centers in LuAG:Ce ceramics is a viable materials-design strategy for enhancing the luminous performance of laser-driven lighting devices.
Despite the success of using Al2O3 as a secondary phase in Ce:LuAG phosphor ceramics (PCs), there is still room for improvement in the compositional design of biphasic PCs, as well as in their luminescent and thermal performance. In this study, nanopowders with 40 wt.% Al2O3-0.4at.% Ce:LuAG stoichiometry were synthesized via a co-precipitation approach. Subsequently, a series of compositionally uniform PCs was successfully fabricated by adjusting the vacuum sintering temperature and dwelling time. The grain size distributions of the Al2O3 and LuAG phases, as well as the evolution of porosity and pore size, were systematically analyzed and correlated with the sintering conditions. The addition of Al2O3 has been demonstrated to enhance the thermal properties of ceramics. The thermal conductivity of the “1750 °C × 10 h” sample was 15.6 W·m−1·K−1 at room temperature. Concurrently, it exhibited excellent thermal quenching behavior, retaining 96% of its luminescence intensity upon heating to 450 K. Its fluorescence lifetime was determined to be 21.06 ns. Under 450 nm laser excitation, the optimized PC attained a luminous efficacy of 286 lm·W−1 at 1 W·mm−2. In addition, the luminous flux increased continuously with laser power from 1 to 20 W·mm−2 without any sign of saturation, reaching a maximum of 2500 lm. The findings indicate that biphasic 40 wt.% Al2O3-0.4at.% Ce:LuAG PCs have potential as high-flux, green-color converters for next-generation high-power laser lighting. Furthermore, a laser illumination prototype device incorporating 40 wt.% Al2O3-0.4at.% Ce:LuAG ceramic samples and a 10 W blue laser was constructed. This device emits white light with an illumination range exceeding 500 m, thereby demonstrating its potential applications in laser-driven lighting.