Clarifying the influence of the dress process parameters of the abrasive water jet on the dressing effect of fixed-abrasive pads (FAPs) is a prerequisite for online controllable dressing of abrasive water jets. This paper uses three factors and three horizontal response surface methods to explore the influence of jet pressure, abrasive concentration, and nozzle angle on FAP dressing quality. The prediction model of the material removal rate of a FAP machined using three process parameters is established. The influence of pairwise interactions of the three process parameter variables on the dressing effect and the optimal process parameters under each target is analyzed. Finally, the optimal process parameters predicted by the model are verified by experiments. The results show that the best dressing parameters with the MRR of the workpiece as the response value are as follows: jet pressure 3.8 MPa, abrasive concentration 3%, and nozzle angle 73°. The predicted value of the optimal process performance is 464.574 nm/min, and the experimental verification result is 469.136 nm/min; the error between the experimental value and the predicted value is within a reasonable range.
Compared to conventional polishing methods, magnetorheological polishing has no subsurface damage and a has good polishing effect, which is suitable for fused silica glass surface processing. However, the existing magnetorheological polishing material removal model has low processing efficiency and uneven removal, which cannot realize the deterministic processing of parts. The material removal (MR) model of fused silica glass is established by convolving the dwell time with the material removal function. The residence time is Fourier transformed. The consequence of process variable such as machining time, workpiece rotational frequency, machining gap and X-direction deflection on the MR of workpiece interface are analyzed. Experiments verify the validity of the material removal model. The surface precision PV value of the workpiece surface under the optimal process parameters was decreased from 7.959 nm to 0.609 nm for machining. The experiment results indicate that the established MR model can be implemented as the deterministic MR of the optical surface and ameliorate the surface accuracy of the workpiece surface.
13 October 2026 in Journal of Materials Engineering and Performance