Elderly falls are a major concerning threat resulting in over 1.5–2 million elderly people experiencing severe injuries and 1 million deaths yearly. Falls experienced by Elderly people may lead to a long‐term negative impact on their physical and psychological health conditions. Major healthcare research had focused on this lately to detect and prevent the fall. In this work, an Artificial Intelligence (AI) edge computing based wearable device is designed and developed for detection and prevention of fall of elderly people. Further, the various deep learning algorithms such as Convolutional Neural Network (CNN), Recurrent Neural Network (RNN), Long Short-Term Memory (LSTM), Gated Recurrent Unit (GRU) are utilized for activity recognition of elderly. Also, the CNN-LSTM, RNN-LSTM and GRU-LSTM with and without attention layer respectively are utilized and the performance metrics are analyzed to find the best deep learning model. Furthermore, the three different hardware boards such as Jetson Nano developer board, Raspberry PI 3 and 4 are utilized as an AI edge computing device and the best deep learning model is implemented and the computation time is evaluated. Results demonstrate that the CNN-LSTM with attention layer exhibits the accuracy, recall, precision and F1_Score of 97%, 98%, 98% and 0.98 respectively which is better when compared to other deep learning models. Also, the computation time of NVIDIA Jetson Nano is less when compared to other edge computing devices. This work appears to be of high societal relevance since the proposed wearable device can be used to monitor the activity of elderly and prevents the elderly falls which improve the quality of life of elderly people.
The increasing demand for sustainable materials has intensified efforts to enhance the performance of recycled polymers for engineering applications. This study investigates the effect of nanoclay reinforcement on the mechanical properties of recycled high-density polyethylene (rHDPE). Nanoclay was incorporated into rHDPE at varying loadings through melt blending, and the resulting composites were evaluated in terms of tensile, flexural, impact, and hardness properties. The tensile strength and tensile modulus improved significantly with increasing nanoclay content, reaching maximum values of 31.27 MPa and 2.39 GPa, respectively, at 1.5 wt% nanoclay, corresponding to increases of 23.11% and 47.53% relative to unreinforced rHDPE. Similarly, the flexural strength and flexural modulus attained peak values of 25.88 MPa and 1105.08 MPa at 1.5 wt% nanoclay, representing improvements of 12.57% and 15.49%, respectively. Impact strength exhibited a different trend, achieving a maximum value of 73.58 kJ/m2 at 0.5 wt% nanoclay before decreasing at higher loadings, indicating a transition towards more brittle behaviour. Hardness increased progressively with nanoclay addition and reached a maximum value of 68.06 Shore D at 1.5 wt%, exceeding both unreinforced rHDPE and virgin HDPE. The overall results demonstrate that nanoclay effectively compensates for the mechanical degradation associated with recycling by enhancing stiffness, strength, and surface hardness. Among the investigated formulations, 1.5 wt% nanoclay provided the optimum balance of mechanical performance, while higher loadings led to reduced reinforcement efficiency due to particle agglomeration. These findings highlight the potential of nanoclay-reinforced rHDPE as a sustainable, high-performance material for applications in packaging, construction, and automotive components, thereby supporting circular economy initiatives and resource-efficient material development.
Fused deposition modelling (FDM) is increasingly used to produce high-performance polymer components; however, the mechanical performance of printed parts is often limited by weak interlayer adhesion, void formation, and residual thermal stresses. In this study, the effects of nozzle temperature, bed temperature, and post-treatment annealing temperature on the tensile and flexural strength of FDM-printed polyether ether ketone (PEEK) were investigated and optimized using Response Surface Methodology (RSM). A face-centred central composite design was employed to evaluate the individual, quadratic, and interaction effects of the three thermal parameters. The results showed that post-treatment annealing temperature was the most influential factor, contributing 56.48% to tensile strength and 52.73% to flexural strength, followed by nozzle temperature, which contributed 30.56% and 30.15%, respectively. Bed temperature showed a comparatively smaller individual effect; however, its interaction with nozzle temperature significantly influenced both tensile and flexural strength. The confirmation experiment performed at 200 °C post-treatment temperature, 414 °C nozzle temperature, and 142 °C bed temperature produced a tensile strength of 55.65 MPa and a flexural strength of 81.08 MPa, with prediction errors of 5.63% and 4.08%, respectively. SEM fracture analysis provided qualitative evidence that improved thermal processing reduced interlayer separation and visible void-related defects while promoting a more cohesive fracture morphology. These improvements are attributed to enhanced interlayer fusion, possible polymer-chain diffusion across layer boundaries, and thermal-stress relaxation during annealing. The findings demonstrate that thermal-parameter optimization and post-treatment annealing can improve the mechanical performance of FDM-printed PEEK within the investigated processing window.