In this paper, a solar cell based on /CdTe heterojunction was analyzed and optimized, for which the following structure of the Al/AZO//CdTe/NiO/Ni device was proposed, which was numerically simulated by the SCAPS 1-D software. Using the software, the effect of the thickness and carrier concentration of the absorber layer (CdTe) and the window layer () was analyzed, and the optimal value of these parameters was found to be 2 µm and for the CdTe layer and 10 nm and for the layer, respectively. The influence of the defect density of the /CdTe interface on the performance of the proposed cell was also analyzed, simulating from to , obtaining better device performance at lower interface defect density. Another parameter analyzed was the operating temperature on the photovoltaic performance of the device, observing that the solar cell has a better performance at lower temperatures. Finally, a maximum optimized PCE of 19.87% is obtained with a Voc = 0.85 V, Jsc = 28.45 , and FF = 82.03%, which makes the /CdTe heterojunction an interesting alternative for the development of CdTe-based solar cells.
GaN films doped with Mg or Zn were obtained via radio-frequency magnetron sputtering on silicon substrates at room temperature and used laboratory-prepared targets with Mg-doped or Zn-doped GaN powders. X-ray diffraction patterns showed broadening peaks, which could have been related to the appearance of nano-crystallites with an average of 7 nm. Scanning electron microscopy and transmission electron microscopy showed good adherence to silicon non-native substrate, as well as homogeneity, with a grain size average of 0.14 µm, and 0.16 µm for the GaN films doped with Zn or Mg, respectively. X-ray photo-electron spectroscopy demonstrated the presence of a very small amount of magnesium (2.10 mol%), and zinc (1.15 mol%) with binding energies of 1303.18, and 1024.76 eV, respectively. Photoluminescence spectrum for the Zn-doped GaN films had an emission range from 2.89 to 3.0 eV (429.23–413.50 nm), while Mg-doped GaN films had an energy emission in a blue-violet band with a range from 2.80 to 3.16 eV (443.03–392.56 nm). Raman spectra showed the classical vibration modes A1(TO), E1(TO), and E2(High) for the hexagonal structure of GaN.
In this work, optical–structural and morphological behavior when Nd is incorporated into ZnO is studied. ZnO and Nd-doped ZnO (ZnO-Nd) films were deposited at 900 °C on Silicon n-type substrates (100) by using the Hot Filament Chemical Vapor Deposition (HFCVD) technique. For this, pellets were made by from powders of ZnO(s) and a mixture of ZnO(s):Nd(OH)3(s). The weight percent of the mixture ZnO:Nd(OH)3 in the pellet is 1:3. The gaseous precursor generation was carried out by chemical decomposition of the pellets using atomic hydrogen which was produced by a tungsten filament at 2000 °C. For the ZnO film, diffraction planes (100), (002), (101), (102), (110), and (103) were found by XRD. For the ZnO-Nd film, its planes are displaced, indicating the incorporation of Nd into the ZnO. EDS was used to confirm the Nd in the ZnO-Nd film with an atomic concentration (at%) of Nd = 10.79. An improvement in photoluminescence is observed for the ZnO-Nd film; this improvement is attributed to an increase in oxygen vacancies due to the presence of Nd. The important thing about this study is that by the HFCVD method, ZnO-Nd films can be obtained easily and with very short times; in addition, some oxide compounds can be obtained individually as initial precursors, which reduces the cost compared to other techniques. Something interesting is that the incorporation of Nd into ZnO by this method has not yet been studied, and depending on the method used, the PL of ZnO with Nd can increase or decrease, and by the HFCVD method the PL of the ZnO film, when Nd is incorporated, increases more than 15 times compared to the ZnO film.
Mg-Zn co-dopedGaN powders via the nitridation of a Ga-Mg-Zn metallic solution at 1000 °C for 2 h in ammonia flow were obtained. XRD patterns for the Mg-Zn co-dopedGaN powders showed a crystal size average of 46.88 nm. Scanning electron microscopy micrographs had an irregular shape, with a ribbon-like structure and a length of 8.63 µm. Energy-dispersive spectroscopy showed the incorporation of Zn (Lα 1.012 eV) and Mg (Kα 1.253 eV), while XPS measurements showed the elemental contributions of magnesium and zinc as co-dopant elements quantified in 49.31 eV and 1019.49 eV, respectively. The photoluminescence spectrum showed a fundamental emission located at 3.40 eV(364.70 nm), which was related to band-to-band transition, besides a second emission found in a range from 2.80 eV to 2.90 eV (442.85–427.58 nm), which was related to a characteristic of Mg-doped GaN and Zn-doped GaN powders. Furthermore, Raman scattering demonstrated a shoulder at 648.05 cm−1, which could indicate the incorporation of the Mg and Zn co-dopants atoms into the GaN structure. It is expected that one of the main applications of Mg-Zn co-doped GaN powders is in obtaining thin films for SARS-CoV-2 biosensors.
Mg-Zn co-doped GaN films were deposited by radio-frequency magnetron sputtering in an N2-Ar2 environment at room temperature, using a target prepared with Mg-Zn co-doped GaN powders. X-ray diffraction patterns showed broad peaks with an average crystal size of 13.65 nm and lattice constants for a hexagonal structure of a = 3.1 Å and c = 5.1 Å. Scanning electron microscopy micrographs and atomic force microscopy images demonstrated homogeneity in the deposition of the films and good surface morphology with a mean roughness of 1.1 nm. Energy-dispersive spectroscopy and X-ray photoelectron spectroscopy characterizations showed the presence of gallium and nitrogen as elemental contributions as well as of zinc and magnesium as co-doping elements. Profilometry showed a value of 260.2 nm in thickness in the Mg-Zn co-doped GaN films. Finally, photoluminescence demonstrated fundamental energy emission located at 2.8 eV (430.5 nm), which might be related to the incorporation of magnesium and zinc atoms.