Artificial neural networks (ANNs) have been an important approach for predicting the value of flow stress, which is dependent on temperature, strain, and strain rate. However, there is still a lack of sufficient knowledge regarding what structure of ANN should be used for predicting metal flow stress. In this paper, we train an ANN for predicting flow stress of In718 alloys at high temperatures using our experimental data, and the structure of the ANN is optimized by comparing the performance of four ANNs in predicting the flow stress of In718 alloy. It is found that, as the size of the ANN increases, the ability of the ANN to retrieve the flow stress results from a training dataset is significantly enhanced; however, the ability to predict the flow stress results absent from the training does not monotonically increase with the size of the ANN. It is concluded that the ANN with one hidden layer and four nodes possesses optimized performance for predicting the flow stress of In718 alloys in this study. The reason why there exists an optimized ANN size is discussed. When the ANN size is less than the optimized size, the prediction, especially the strain dependency, falls into underfitting and fails to predict the curve. When the ANN size is less than the optimized size, the predicted flow stress curves with the temperature, strain, and strain rate will contain non-physical fluctuations, thus reducing their prediction accuracy of extrapolation. For metals similar to the In718 alloy, ANNs with very few nodes in the hidden layer are preferred rather than the large ANNs with tens or hundreds of nodes in the hidden layers.
In this study, post-welding aging treatments were applied to a novel Ni-based superalloy GH4065A inertia friction welding (IFW) joint to improve its high-temperature properties. The effect of aging treatment on the microstructure and creep resistance of the IFW joint was systematically investigated. The results indicated that the original precipitates in the weld zone almost completely dissolved during the welding process, and fine tertiary precipitated during the subsequent cooling process. Aging treatment did not significantly change the characteristics of grain structures and primary in the IFW joint. After aging, the size of tertiary in the weld zone and secondary in the base material increased, but their morphology and volume fraction did not change evidently. After 760 °C, 5 h aging treatment, the tertiary in the weld zone of the joint grew from 12.4 nm to 17.6 nm. Correspondingly, the creep rupture time of the joint at 650 °C and 950 MPa increased from 7.51 h to 147.28 h, which is about 19.61 times higher than that of the as-welded joint. The creep rupture was more likely to occur in the base material instead of the weld zone for the IFW joint. This revealed that the creep resistance of the weld zone was significantly improved after aging due to the growth of . However, increasing the aging temperature or extending the aging time promoted the growth of secondary in the base material, and meanwhile, M23C6 carbides tended to continuously precipitate at the grain boundaries of the base material. It might decrease the creep resistance of the base material.
Nickel-based superalloys are indispensable in aerospace engines due to their exceptional high-temperature strength, oxidation resistance, and corrosion resistance, making them critical for joining processes such as inertia friction welding (IFW), which is favored for its efficiency and superior joint quality. In this study, IFW was used to join FGH101 powder superalloy with IN718 deformed superalloy, resulting in significant plastic deformation that formed symmetrical ear-shaped flash on the IN718 side and minor upsetting on the FGH101 side, with a wavy interface due to heat dissipation. Microhardness analysis revealed higher hardness at the weld interface, followed by a sharp decline near the Heat Affected Zone (HAZ) on the IN718 side due to phase re-dissolution, while FGH101 showed quicker recovery. Post-weld aging treatments enhanced hardness and strength through γ′ and δ phase precipitation in FGH101 and γ″ phases in IN718. Room temperature tensile tests demonstrated impressive strength with failures occurring plastically within the IN718 base metal, whereas elevated temperatures shifted failure locations to the weld zone without necking. Fatigue tests exhibited varied lifespans, with fractures initiating either at stress concentrators or within the FGH101 base metal far from the weld center. Scanning electron microscope (SEM) analysis confirmed mixed-mode fracture patterns, underscoring the importance of microstructure on joint performance and suggesting that optimizing IFW parameters can lead to superior weld quality in aerospace components, thus providing valuable insights for future research and industrial applications.
The welded joint of a dissimilar titanium alloy was obtained via inertial friction welding technology. The characteristics of the bonding interface and the microstructure of the welded joint were investigated via optical microscopy, scanning electron microscopy and electron backscattered diffraction. The results show that fine, equiaxed grains and interdiffusion bands of the elements Mo and Sn were formed in the weld zone under the high temperature and plastic deformation of the inertial friction welding. The weld zone and thermo-mechanically affected zone formed α texture and β texture, respectively.
As a major load-bearing component of trains, the weld quality of the bogie beam is critical to the safety of railway operations. This study specifically investigates the inertia friction welding process of S355 bogie crosshead tubes, with the aim of improving the weld quality and achieving one-time formation of the crosshead tube and tube seat. The microstructural features and mechanical properties of S355 inertia-welded joints were also compared with the base metal. Research indicates that inertia friction welds have no visible defects, and that the microstructure of the welding seam (WS) consists of granular bainite, acicular ferrite and little pearlite. The thermo-mechanically affected zone (TMAZ) consists of granular bainite bands and ferrite + pearlite bands. The hot work strengthening mechanism of inertia friction welding results in a higher level of hardness for both WS and TMAZ. The tensile property of the welded joints can be compared to the base metal. The yield strength, tensile strength and elongation of the welded joints, respectively, reach 87.5%, 100% and 79.5% of S355. However, the impact toughness of the welds at room temperature is lower than that of the base material, particularly in the TMAZ zone. Conversely, in an environment with a temperature of −40 °C, WS’s impact toughness surpasses that of the parent material.