Decarbonization of non-metallic mineral manufacturing requires reductions in energy use relative to output alongside changes in fuel use and production processes. This study examines associations between energy intensity, energy structure, and production-based CO2 intensity in the EU non-metallic mineral sector (NACE C23). A balanced panel of 19 Member States (2008–2023) is analyzed using static and dynamic two-way fixed-effects models complemented by additive Logarithmic Mean Divisia Index (LMDI) decomposition. Energy intensity is positively associated with CO2 intensity in the fixed-effects specifications, whereas relationships with electricity and fossil-fuel shares are less consistent. Dynamic estimates suggest positive CO2-intensity persistence, but its magnitude is sensitive to estimator choice. Across annual country-level transitions, the LMDI energy-intensity effect has the largest average downward contribution to changes in absolute CO2 emissions (−267.75 kt), followed by the fossil-fuel-share effect (−117.24 kt). Subperiod analysis reveals temporal heterogeneity: fossil-fuel share contributed more strongly in 2008–2014, whereas energy intensity dominated in 2015–2019 and 2020–2023. These findings distinguish energy-intensity adjustment from energy-carrier substitution as complementary dimensions of industrial decarbonization. Because sectoral emissions may include process-related CO2 and exclude indirect electricity emissions, the results do not establish the carbon benefits of electrification or specific technological changes.
The operating temperature of a photovoltaic module strongly affects its electrical performance, while direct temperature measurements may be influenced by sensor placement, thermal resistance, and measurement delay. This paper investigates the use of open-circuit voltage for estimating the temperature of a photovoltaic module under varying irradiance conditions. Two standard-based approaches, derived from IEC 60904-5 and EN 50530, are compared with a proposed empirical model in which the temperature sensitivity of the open-circuit voltage is allowed to vary with irradiance. The experimental study was carried out using a water-cooled 10 W polycrystalline PV module. A total of 135 I–V characteristics were measured at 15 irradiance levels between 72 and 834 W/m2 and at nine module temperatures between 30 and 70 °C. The parameters of all investigated models were identified from the experimental data, and their temperature estimation performance was evaluated over the complete measurement range. The standard-based methods provided satisfactory results mainly at medium and high irradiance levels, whereas their accuracy decreased at low irradiance. The proposed model accounted for the irradiance dependence of the open-circuit voltage temperature sensitivity and reduced the estimation error over the investigated operating range. The obtained RMSE was 0.26 °C, with a mean absolute error of 0.21 °C and a maximum absolute error of 0.82 °C. These results indicate that the proposed approach can provide a simple method for indirect PV module temperature estimation in monitoring and control applications.
Ion-exchange-strengthened 0.7 mm aluminosilicate glass offers a promising route to lightweight, mechanically robust front covers for building-integrated photovoltaic (BIPV) modules, but systematic characterization at sub-millimeter thicknesses remains limited. This study investigated 100 × 60 × 0.7 mm glass samples subjected to Na+/K+ ion exchange (6 h, 430 °C, KNO3) and characterized mechanical and optical properties relevant to BIPV applications. Depth of layer (DOL) was cross-validated using three independent methods, mass gain diffusion modeling (31–37 μm), elasto-optic measurements (FSM-6000: 38–42 μm), and EDS Na/K depth profiling (35–40 μm), confirming consistent strengthened layer depth of 35–40 μm. Surface compressive stress measured 733 MPa (Series 2) and 773 MPa (Series 3), significantly exceeding conventional PV cover glass (490–515 MPa, 1 mm thickness). Vickers hardness increased by 17.7% (490 → 596 HV, p < 0.0001), demonstrating enhanced damage tolerance. Spectrophotometric analysis (200–2400 nm) showed transmittance >91% (380–2000 nm) and >92% (600–2000 nm) for both as-received and strengthened glass, confirming no optical degradation (p = 0.29–0.41). The 78–83% mass reduction relative to standard 3.2–4 mm glass, combined with superior CS/DOL and preserved optical performance, establishes ion-exchanged 0.7 mm aluminosilicate glass as a strong material-level candidate for next-generation lightweight BIPV modules. Future work requires module-scale mechanical validation (bending, impact testing per EN/IEC standards) and techno-economic assessment to verify system-level benefits.