The β-Ti alloys have attracted the attention of researchers due to their excellent properties and their remarkable biocompatibility. The present study evaluated the mechanical behavior analysis (hardness, compressive strength, and modulus of elasticity) of the Ti-15Mo-W system. For experimental research, we chose the TiMo15 biocompatible alloy as a starting material. In order to improve the mechanical properties, we added tungsten amounts of 3.88 to 12.20 wt.% and analyzed the results obtained. The successive melting of the samples was done using a vacuum arc furnace in a copper crucible cooled with water. Following micro-structural investigations, we found this alloy possessed a homogeneous structure and showed β-phase predominance. The investigated alloys have good mechanical properties—the mean Vickers micro-hardness values are between 251 to 321 HV, the compressive strength values range from 717 to 921 MPa, and the modulus of elasticity is between 17.86 and 45.35 GPa. These results are compatible to the requirements of a metallic material for medical applications as artificial implant devices.
The Bi-Sn, Bi-Sn-Ag, and Bi-Sn-Sb solder alloy systems represent lead-free, environmentally friendly alternatives for reliable electronic assembly. These alloys comply with increasingly strict environmental and health regulations, while offering low melting points suitable for soldering temperature-sensitive components. Microstructural analysis revealed distinct phase segregation in all alloys, with Sb promoting coarse Sn2Sb3 intermetallic compounds and Ag inducing fine needle-like Ag3Sn precipitates. Eutectic refinement and compositional contrast were confirmed by SEM-BSE and EDS mapping. Vickers microhardness measurements revealed increased hardness in Sb- and Ag-modified Bi–Sn alloys, with Ag3Sn dispersion yielding the highest strengthening effect, indicating enhanced mechanical potential. This study also reports the thermal and electrical conductivities of Bi60Sn40, Bi60Sn35Ag5, and Bi60Sn35Sb5 alloys over the 25–140 °C range. Bi60Sn40 showed an increase in thermal conductivity across the full temperature range from 16.93 to 26.93 W/m·K, while Bi60Sn35Ag5 reached 18.28 W/m·K at 25 °C, and Bi60Sn35Sb5 exhibited 13.90 W/m·K. These findings underline the critical influence of alloying elements on microstructure, phase stability, and thermophysical behavior, supporting their application in low-temperature soldering technologies.
27 June 2017 in IOP Conference Series: Materials Science and Engineering
In this work, the depleted active paste from spent lithium–ion batteries was separated from cathode by means of ultrasonic vibration. First the unit cells were discharged in brine at room temperature, for safety reasons. Then anode, separator, electrolyte and cathode were separated. Spent Li-Ion batteries were introduced into a washing container to separate electrode materials from their support substrate: active paste (lithium cobalt oxide – LiCoO2) from cathode (Al foil) and graphite from anode (Cu foil). The Al foil and Cu foil were also recovered. A cleaning efficiency of 91% was achieved using a solution of 1.5 M acetic acid after a 6 minute time of exposure into an ultrasonic washing container with a frequency and electric power of 50 kHz and 50 W, respectively. The XRD patterns and the morphology of LiCoO2 powder were presented.
The experimental research was focused on the investigation of valuable material from spent Ni-MH type AA batteries, namely the metal grid anodes and the black mass material (anode and cathode powder). The materials of interest were analyzed by X-ray fluorescence spectroscopy (XRF), ICP-OES (inductively coupled plasma optical emission spectrometry), optical microscopy, scanning electron microscopy (SEM), energy-dispersive X-ray analysis (EDX), electron backscatter diffraction (EBSD), and X-ray diffraction (XRD). The analyzed grids have a high Fe content, but some of them correspond to the Invar alloy with approx. 40% Ni. In the black mass material, round particles and large aggregations were observed by SEM analysis, showing a high degree of degradation. The XRD analysis reveals the presence of only three compounds or phases that crystallize in the hexagonal system: La0.52Ce0.33Pr0.04Nd0.11Co0.6Ni4.4, Ni(OH)2, and La5Ni19. The obtained results provide useful and interesting information that can be used for further research in the recycling and economic assessment of metals from spent Ni-MH batteries.