Three benzo[1,2-b:4,5-b′]dithiophene (BDT)-based donor–acceptor (D–A) conjugated polymers with different side chains were designed, synthesized, and investigated as organic thermoelectric materials. Changing the side chains caused the three polymers to have different physical and chemical properties. The thermoelectric properties of BDT-based conjugated polymers have been systematically investigated through fine tuning of the side chains. Among the three polymers, the polymer with alkylthienothiophene moieties as the side chains exhibited the best thermal stability (thermal decomposition temperature above 400 °C), the highest electrical conductivity (1.519 S cm−1), and the largest Seebeck coefficient (413.79 μV K−1). The results of this study can guide the future design and synthesis of high-performance thermoelectric conjugated polymers.
3 April 2019 in Macromolecular Rapid Communications
Although lithium–sulfur (Li–S) batteries are a promising secondary power source, it still faces many technical challenges, such as rapid capacity decay and low sulfur utilization. The loading of sulfur and the weight percentage of sulfur in the cathode usually have a significant influence on the energy density. Herein, we report an easy synthesis of a self-supporting sulfur@graphene oxide-few-wall carbon nanotube (S@GO–FWCNT) composite cathode film, wherein an aluminum foil current collector is replaced by FWCNTs and sulfur particles are uniformly wrapped by graphene oxide along with FWCNTs. The 10 wt% FWCNT matrix through ultrasonication not only provided self-supporting properties without the aid of metallic foil, but also increased the electrical conductivity. The resulting S@GO–FWCNT composite electrode showed high rate performance and cycle stability up to ∼385.7 mA h gelectrode−1 after 500 cycles and close to ∼0.04% specific capacity degradation per cycle, which was better than a S@GO composite electrode (353.1 mA h gelectrode−1). This S@GO–FWCNT composite self-supporting film is a promising cathode material for high energy density rechargeable Li–S batteries.
Polymer/inorganic thermoelectric composites have witnessed rapid progress in recent years, but most of the studies have focused on the traditional conducting polymers. The limited structures of traditional conducting polymers restrain the development of organic thermoelectric composites. Herein, we report the preparation and thermoelectric properties of a series of composites films based on SWCNTs and bipyridine-containing polyfluorene derivatives. The value of the power factor around 12 μW m−1 K−2 was achieved for the composite F8bpy/SWCNTs with a mass ratio of 50/50, and the maximum value of 62.3 μW m−1 K−2 was obtained when the mass ratio reached 10/90. Moreover, taking advantage of the bipyridine unit could chelate various kinds of metal ions to form polymer complexes. The enhanced power factor of 87.3 μW m−1 K−2 was obtained for composite F8bpy-Ni/SWCNTs with a mass ratio of 50/50. Finally, the thermoelectric properties of the bipyridine-containing polyfluorene derivative/SWCNT composites were conveniently tuned by chelating with different metal ions.
In the development of wearable electronic devices, the composite modification of conductive polymers and single-walled carbon nanotubes (SWCNTs) has become a burgeoning research area. This study presents the synthesis of a novel polythiophene derivative, poly(3-alkoxythiophene) (P3(TEG)T), with alkoxy side chains. Different molecular weight variants of P3(TEG)T (P1–P4) were prepared and combined with SWCNTs to form composite materials. Density functional theory (DFT) calculations revealed a reduced bandgap for P3(TEG)T. Raman spectroscopy demonstrated π-π interactions between P3(TEG)T and SWCNTs, facilitating the dispersion of single-walled carbon nanotubes and the formation of a continuous conductive network. Among the composite films, P4/SWCNTs-0.9 exhibited the highest thermoelectric performance, with a power factor (PF) value of 449.50 μW m−1 K−2. The fabricated flexible thermoelectric device achieved an output power of 3976.92 nW at 50 K, with a tensile strength of 59.34 MPa for P4/SWCNTs. Our findings highlight the strong interfacial interactions between P3(TEG)T and SWCNTs in the composite material, providing an effective charge transfer pathway. Furthermore, an improvement in the tensile performance was observed with an increase in the molecular weight of the polymer used in the composite, offering a viable platform for the development of high-performance flexible organic thermoelectric materials.
Composite films of indacenodithiophene-bezothiadazole copolymers bearing polar side chains (P1) and single wall carbon nanotubes (SWCNTs) are found to show a competitive thermoelectric performance compared to their analogous polymers with aliphatic side chains (P2). The enhanced power factors could be attributed to the stronger interfacial interactions between the P1/SWCNTs compared to that of P2/SWCNTs containing the same ratio of SWCNTs. A maximum power factor of 161.34 μW m−1 K−2 was obtained for the composite films of P1/SWCNTs for a filler content of 50 wt%, which is higher than that of P2/SWCNTs (139.06 μW m−1 K−2, 50 wt%). Our work sheds light on the design of side-chains in efficient conjugated polymers/SWCNTs thermoelectric materials and contributes to the understanding of their thermoelectric properties.