Polymer/inorganic thermoelectric composites have witnessed rapid progress in recent years, but most of the studies have focused on the traditional conducting polymers. The limited structures of traditional conducting polymers restrain the development of organic thermoelectric composites. Herein, we report the preparation and thermoelectric properties of a series of composites films based on SWCNTs and bipyridine-containing polyfluorene derivatives. The value of the power factor around 12 μW m−1 K−2 was achieved for the composite F8bpy/SWCNTs with a mass ratio of 50/50, and the maximum value of 62.3 μW m−1 K−2 was obtained when the mass ratio reached 10/90. Moreover, taking advantage of the bipyridine unit could chelate various kinds of metal ions to form polymer complexes. The enhanced power factor of 87.3 μW m−1 K−2 was obtained for composite F8bpy-Ni/SWCNTs with a mass ratio of 50/50. Finally, the thermoelectric properties of the bipyridine-containing polyfluorene derivative/SWCNT composites were conveniently tuned by chelating with different metal ions.
27 June 2025 in Journal of Colloid and Interface Science
In this study, a benzodithiophene (BDT)-based donor (D)–acceptor (A) polymer containing carbazole segment in the side-chain was designed and synthesized and the thermoelectric composites with 50 wt % of single walled carbon nanotubes (SWCNTs) were prepared via ultrasonication method. Strong interfacial interactions existed in both of the composites before and after immersing into the 2,3,5,6-Tetrafluoro-7,7,8,8-tetracyanoquinodimethane (F4TCNQ) solution as confirmed by UV-Vis-NIR, Raman, XRD and SEM characterizations. After doping the composites by F4TCNQ, the electrical conductivity of the composites increased from 120.32 S cm−1 to 1044.92 S cm−1 in the room temperature. With increasing the temperature, the electrical conductivities and Seebeck coefficients of the undoped composites both decreased significantly for the composites; the power factor at 475 K was only 6.8 μW m−1 K−2, which was about nine times smaller than the power factor at room temperature (55.9 μW m−1 K−2). In the case of doped composites, although the electrical conductivity was deceased from 1044.9 S cm−1 to 504.17 S cm−1, the Seebeck coefficient increased from 23.76 μV K−1 to 35.69 μW m−1 K−2, therefore, the power factors of the doped composites were almost no change with heating the composite films.