The structural, optical, and electrical properties of zinc oxide (ZnO) layers manufactured at different process conditions were investigated. ZnO epitaxial layers were grown on silicon, glass, and ITO/glass substrates by pulsed laser deposition (PLD) technique. The influence of power beam, substrate temperature, and deposition time on films properties was analysed. Morphological features of the film surface were investigated by scanning electron microscopy. A structural study shown planar orientation of films at low temperatures of substrate, but the columnar type of growth originated in temperature enhances. Electrical properties were determined in the temperature range 300–500 K. It was shown that the type of films conductivity is metallic and it is limited by charge transfer across grain boundaries.
The local density approximation has been implemented to determine the band structure of orthorhombic crystals (YAP) and SbSI. The topology of the valence band structures was analyzed. It has been demonstrated that Zak’s elementary energy bands in the band structure are distinguishable on the basis of the empty-lattice approximation. The calculated electron density distribution of YAP and SbSI crystals is related to particular Wyckoff positions. Moreover, there is a direct correspondence between the obtained elementary energy bands and the aforementioned Wyckoff positions characterized by electron density distribution.
Several Cu2O and TiO2 thin films and four additional TiO2/Cu2O structures were fabricated by direct current (DC) magnetron sputtering. The process parameters were selected on the basis of earlier studies and numerical simulations. We examined the morphology of a cross-section of the PV structures, roughness and topography, and the transmission spectra of the thin films. Additionally, the properties of the samples were determined by X-ray diffraction. Next, the morphology cross-sectional and layer compositions of the solar cells was evaluated by scanning electron microscopy. Only one of the TiO2/Cu2O structures appeared smooth and homogeneous with columnar-type growth. For the as-grown films, diffraction peaks were observed and identified as brookite, rutile, CuO, and Cu2O and the average roughness of the samples was 0.5, 1.2, 5.4, and 4.0 nm, respectively. Finally, the transmission spectra of the thin films were recorded. Transmission and reflection spectra of ultraviolet-visible spectroscopy were analyzed, and the optical band gap and absorption coefficient of the oxidized layers were calculated. In the region of 400 to 1000 nm, transmittance varied from 5% to 70% in the TiO2 samples, and from 15% to 40% in the Cu2O samples, and reflectance of the TiO2 and Cu2O samples ranged from 20% to 90%. In the region of 1.5 eV to 3.5 eV, the mean absorption coefficient varied from ∼105 1/cm to ∼3 · 105 1/cm for TiO2 thin film, and from ∼2 · 105 to ∼6 · 105 1/cm for Cu2O thin film. The optical band gap values of the samples shifted slightly toward bulk anatase-3.5 eV, bulk rutile-3.1 eV, and copper(I) oxide. Finally, silver contacts were used for the electrodes. One of the fabricated TiO2/Cu2O PV structures was found to be sensitive to electromagnetic radiance during the experiment.