The properties of Al-Cu-Mg alloys simultaneously depend on dissolving the maximum amount of Cu and Mg in the solution treatment and on achieving optimal ageing. The aim of this study is to analyze the effect on an Al-Cu4.5-Mg1.5-Si0.75 alloy, manufactured by continuous casting and hot rolling until achieving a reduction in its cross-section greater than 90%, of the dwell time at the solution temperature, 495 °C (4, 8, and 24 h), of the different ageing temperatures (160, 180, and 200 °C), and of cold rolling prior to ageing. The microstructural variations underwent the material during its manufacturing process, form its continuous casting to subsequent hot rolling, were analyzed by means of optical microscopy (OM) and scanning electronic microscopy (SEM), with characteristic energy dispersive X-ray (EDX) microanalysis. The crystalline phases present after the different solution and natural ageing treatments were identified and quantified by means of X-ray diffraction (XRD), concluding that Mg is easier to dissolve than Cu. The transient states associated with the Mg2Si phase are the most abundant. However, the longer the dwell time at the solution temperature, the greater the weight percentage of the transient states associated with the Al2Cu phase during ageing. The higher the ageing temperature, the faster the peak hardness is reached, but the lower its value. The ageing temperature that allows the highest hardness to be obtained was 160 °C. The maximum hardness value reached was 162 HV, obtained after a solution treatment at 495 °C for 4 h and ageing at 160 °C for 50 h. By means of prior cold rolling, the peak hardness values are reached more quickly and their values slightly exceed those obtained without this deformation. With ageing at 180 °C, 168 HV are reached after 6 h at this temperature.
High intensity shot peening treatments have been combined with other different second treatments, such as low intensity shot peening, vibratory finishing and grit blasting with fine alumina powders, in order to optimize the fatigue life of a medium-alloyed, quenched and tempered, structural steel with a very high strength (2000MPa). Single low intensity shot peening treatments using ceramic balls were also used with the same objective.Roughness and residual stress profiles were measured, while the fatigue behavior was analyzed using a rotating bending fatigue equipment. Fracture surfaces were also analyzed in a scanning electron microscope (SEM) and the location of the fatigue crack initiation was detected.Although the maximum stress in our fatigue tests is always applied on the surface of the specimen, the appropriate surface treatment combinations were able to optimize the fatigue response of the steel until the point where the fatigue crack initiated in the specimen interior (subsurface nucleation), due to the microstructural stress concentration provided by small alumina inclusions present in the microstructure of the steel. The amplitude of the stress intensity factor necessary to propagate fatigue cracks in the studied steel and the intrinsic stress intensity factor threshold, ΔKth, were finally obtained
8 February 2018 in The International Journal of Advanced Manufacturing Technology
Böhler K390 steel is used for cold work tools, with 9% of V, made by using powder metallurgy. In this work, it has been studied the effect of shot peening and nitriding surface treatments on wear resistance and impact toughness of this type of steel. For this purpose, previous changes in several thermal processing factors related to quenching and tempering were carried out. The results allow for an increase in the hardness, impact toughness, and abrasive wear resistance of these steels. An austenitizing treatment at 1100 °C with air cooling and 3 tempering processes at 550 °C is suggested. These conditions foster a lower weight percentage of retained austenite, up to 3%, a higher carbide percentage, up to 15–16% in weight, and a greater impact toughness with no notch, of above 40 J/cm2. If this treatment is combined with further ion nitriding, the maximum level of abrasive wear resistance is reached. The only carbide type present in the microstructure is the MC type. Most of the V, Cr, and Mo contents are present in said carbides. The Co and the W tend to remain in solid solution in the matrix constituent. Both the shot peening treatment as well as ion nitriding offer a considerable increase in hardness, with values of up to 1500–1600 HV. Nevertheless, it has been confirmed that shot peening does not offer any abrasive wear resistance improvement. Such resistance may only be considerably improved by the application of an ionic nitriding treatment. The thickness of the nitrided layer fluctuates between 150 and 175 µm. The carbides are affected by nitriding, reaching levels that are higher than the atomic 10%, at an intermediate depth of the nitrided layer. These values are higher in the matrix constituent, as they are even higher than the atomic 20% in N.