Magnetic composites of soft magnetic FeGa particles embedded in a silicone matrix have been synthesized. The Villari effect has been studied depending on the size and concentration of the particles and on the magnetic state of the composite. The results indicate a decrease in the Villari effect when the concentration of the magnetic particles increases. These results suggest a relationship between the Villari effect and the mechanical properties of the composites. The Young’s modulus of the composites has been obtained by microindentation and their values related to the intensity and slope of the Villari signals. The results are explained on the basis that the reduction in the cross section of the composite when submitted to stress is the main origin of the variation of the magnetic flux in the Villari effect in this kind of composite. It has also been obtained that the magnetic state of the composite plays an important role in the Villari signal. When the magnetization of the composite is greater, the magnetic flux across the composite is greater too and, so, the same reduction in the cross section originates a greater Villari signal.
This paper presents the results obtained regarding the control by manufacturers of the percentage, shape, and size of the precipitated graphite in the working layer of duplex work-rolls used in hot strip mill finishing stands. This working layer is manufactured in a martensitic white cast iron alloyed with Cr and Nb to promote the precipitation of M3C and MC carbides, which provide a high wear resistance. The thermal cycling behavior of this layer also has a decisive influence on its service life. In this context, the percentage of graphite and its morphology play a very important role against said thermal cycling. With the aim of studying their effect on the sphericity of graphite, the analyzed industrial manufacturing factors worth highlighting include the liquidus temperature, the %Si, the use of an FeSi inoculant with traces of Lanthanum, inoculation with different amounts of FeB and SiCaMn, and the addition of Mg. At the periphery of the working layer, it was found that the use of the FeSi inoculant with traces of La promoted an increase in the density of counts of graphite, and that inoculation with FeB and the addition of 0.02% Mg diminished the nodularity of the graphite. Furthermore, throughout the entire thickness of the working layer, an increase in the amount of SiCaMn of up to 0.6 kg/T produced an increase in the size of the graphite particles and a marked improvement in their nodularity.
Böhler K390 steel is used for cold work tools, with 9% of V, made by using powder metallurgy. In this work, it has been studied the effect of shot peening and nitriding surface treatments on wear resistance and impact toughness of this type of steel. For this purpose, previous changes in several thermal processing factors related to quenching and tempering were carried out. The results allow for an increase in the hardness, impact toughness, and abrasive wear resistance of these steels. An austenitizing treatment at 1100 °C with air cooling and 3 tempering processes at 550 °C is suggested. These conditions foster a lower weight percentage of retained austenite, up to 3%, a higher carbide percentage, up to 15–16% in weight, and a greater impact toughness with no notch, of above 40 J/cm2. If this treatment is combined with further ion nitriding, the maximum level of abrasive wear resistance is reached. The only carbide type present in the microstructure is the MC type. Most of the V, Cr, and Mo contents are present in said carbides. The Co and the W tend to remain in solid solution in the matrix constituent. Both the shot peening treatment as well as ion nitriding offer a considerable increase in hardness, with values of up to 1500–1600 HV. Nevertheless, it has been confirmed that shot peening does not offer any abrasive wear resistance improvement. Such resistance may only be considerably improved by the application of an ionic nitriding treatment. The thickness of the nitrided layer fluctuates between 150 and 175 µm. The carbides are affected by nitriding, reaching levels that are higher than the atomic 10%, at an intermediate depth of the nitrided layer. These values are higher in the matrix constituent, as they are even higher than the atomic 20% in N.