Predicting the residual life of a structure is an essential issue in structure management. Many researchers have used different methods to predict structure lifetimes, such as the creep rupture test. However, this test is costly and time-consuming, and since it is also destructive, an unused specimen must be tested rather than an actual specimen in use. The instrumented indentation test (IIT), on the other hand, is easier and faster than conventional test methods, most important of all, it is a non-destructive method to obtain mechanical properties that can be performed on the actual structure in use. In this study, we obtained mechanical properties of a SA213-T23 tube material for a thermal power plant degraded for 1~2,000 hours at high temperature. and observed the degradation by analyzing the microstructure. We found a relation between the Larson-Miller Parameter (LMP) and degradation tensile properties considering the temperature and degradation time and suggested a method to predict the residual life by applying a failure criterion. Also, we confirmed that our interaction formula and the residual life are reasonable by comparison with statistical rupture time data from materials that have in fact degraded.
Invar alloy sheet was welded by resistance seam welding (RSW) with a constant electrode force and three different welding currents. Tensile properties were evaluated using instrumented indentation testing (IIT) with a spherical indenter and microstructure observations were obtained under an optical microscope. IIT performed on the base material at room temperature (RT) and −163 °C, a cryogenic temperature (CT), gave results in good agreement with those of tensile testing. The strength of each zone was higher in the order of heat-affected zone (HAZ) < weld nugget (WN) < base material (BM) because the amount of cold working was least in the BM, heavy metal elements and carbon vaporized during melting, and the WN was formed more tightly than the HAZ, effectively constraining the plastic zone generated by the indentation. As for the welding current, the nugget, which becomes larger and tighter as the current increases, more effectively constrained the plastic zone in the indentation, and this soon increased the strength. Generally, Invar is known to consist of single-phase austenite, and microstructure observations have confirmed that the average grain size is ordered as BM < HAZ < WN. Fan-like columnar grains developed in the direction of the temperature gradient, and equiaxed grains were observed near the BM. It was confirmed that the grain size in the WN also increases as the current is increased. Interestingly, the constraint effect with increasing nugget size was more important for strength than the grain size.
31 May 2021 in International Journal of Automotive Technology
SA213 T92 steel is generally used in power plants as a high-temperature structural material. In order to evaluate the degradation of the flow properties of T92 by heat, accelerated tests were conducted at various time-temperature combinations reflecting actual service conditions, and hardness and tensile tests were performed. Observation of the microstructure of accelerated test specimens confirmed that the microstructural change is related to the degradation of flow properties, which can be described by the Hollomon and Jaffe equation.