Aluminium nitride (AlN) is a promising material for challenging sensor applications such as process monitoring in harsh environments (e.g., turbine exhaust), due to its piezoelectric properties, its high temperature stability and good thermal match to silicon. Basically, the operational temperature of piezoelectric materials is limited by the increase of the leakage current as well as by enhanced diffusion effects in the material at elevated temperatures. This work focuses on the characterization of aluminum nitride thin films after post deposition annealings up to temperatures of 1000 °C in harsh environments. For this purpose, thin film samples were temperature loaded for 2 h in pure nitrogen and oxygen gas atmospheres and characterized with respect to the film stress and the leakage current behaviour. The X-ray diffraction results show that AlN thin films are chemically stable in oxygen atmospheres for 2 h at annealing temperatures of up to 900 °C. At 1000 °C, a 100 nm thick AlN layer oxidizes completely. For nitrogen, the layer is stable up to 1000 °C. The activation energy of the samples was determined from leakage current measurements at different sample temperatures, in the range between 25 and 300 °C. Up to an annealing temperature of 700 °C, the leakage current in the thin film is dominated by Poole-Frenkel behavior, while at higher annealing temperatures, a mixture of different leakage current mechanisms is observed.
1 October 2014 in Energy Conversion and Management
Remote interrogation of surface acoustic wave identification tag (ID-tags) imposes a high signal amplitude which is related to a high coupling coefficient value (K2) and low propagation losses (α). In this article, we propose and discuss an alternative configuration to the standard one. Here, we replaced the conventional configuration, i.e., one interdigital transducer (IDT) and several reflectors, by a series of electrically connected IDTs. The goal is to increase the amplitude of the detected signal using direct transmission between IDTs instead of the reflection from passive reflectors. This concept can, therefore, increase the interrogation scope of ID-tags made on a conventional substrate with high K2 value. Moreover, it can also be extended to suitable substrates for harsh environments, such as high-temperature environments: the materials used exhibit limited performances (low K2 value and relatively high propagation losses) and are, therefore, rarely used for identification applications. The concept was first tested and validated using the lithium niobate 128° Y-X cut substrate, which is commonly used in ID-tags. A good agreement between experimental and numerical results was obtained for the promising concept of connected IDTs. The interesting features of the structure were also validated using a langasite substrate, which is well-known to operate at very high temperatures. Performances of both substrates (lithium niobate and langasite) were tested with an in situ RF characterization up to 600°C. Unexpected results regarding
Surface Acoustic Wave (SAW) sensors are small, passive and wireless devices. We present here the latest results obtained in a project aimed at developing a SAW-based implantable pressure sensor, equipped with a well-defined, 30 μm-thick, 4.7 mm-in-diameter, Lithium Niobate (LN) membrane. A novel fabrication process was used to solve the issue of accurate membrane etching in LN. LN/Si wafers were fabricated first, using wafer-bonding techniques. Grinding/polishing operations followed, to reduce the LN thickness to 30 μm. 2.45 GHz SAW Reflective Delay-Lines (R-DL) were then deposited on LN, using a combination of e-beam and optical lithography. The R-DL was designed in such a way as to allow for easy temperature compensation. Eventually, the membranes were etched in Si. A dedicated set-up was implemented, to characterize the sensors versus pressure and temperature. The achieved pressure accuracy is satisfactory (±0.56 mbar). However, discontinuities in the response curve and residual temperature sensitivity were observed. Further experiments, modeling and simulations were used to analyze the observed phenomena. They were shown to arise essentially from the presence of growing thermo-mechanical strain and stress fields, generated in the bimorph-like LN/Si structure, when the temperature changes. In particular, buckling effects explain the discontinuities, observed around 43 °C, in the response curves. Possible solutions are suggested and discussed.