The high magnitude of quench-induced residual stress in thick aluminum plates is attributed not only to high thermal stress but also to high yield strength due to quench-induced precipitation hardening. To date, lowering the thermal stress is the only path to reduce the residual stress in the design of quenching technology. In this paper, a new path is proposed that reduces the residual stress through decreasing the yield strength at ambient temperatures by eliminating the precipitation hardening effect during quenching. As certified in several experiments, the high yield strength of thick as-quenched plates decreases rapidly from a short period of extra heat preservation at relatively higher temperatures. Therefore, an interrupted quenching method is proposed, wherein quenching is interrupted after an initial cooling period and the sample is placed in air to make the temperature field uniform; afterward, the sample is cooled to room temperature. Interrupted quenching tests were conducted on 115 mm thick 7050 aluminum plates and significant residual stress reductions were observed in the specimens compared with the residual stresses in the specimens subjected to regular quenching.
The aim of this study was to predict the yield strength of as-quenched aluminum alloys according to their continuous quench cooling path. Our model was established within the framework of quench factor analysis (QFA) by representing a quenching curve as a series of consecutive isothermal transformation events and adding the yield strength increments after each isothermal step to predict the yield strength after continuous quench cooling. For simplification; it was considered that the effective hardeners during quenching were the nanosized solute clusters formed at low temperatures, whereas the other coarse precipitates were neglected. In addition, quenching tests were conducted on aluminum plates with different thicknesses. The predictions were compared with the experimental measurements, and the results showed that the predictions fit the measurements well for the 40- and 80-mm-thick plates but overestimated the as-quenched yield strength at the mid-thickness of the 115-mm-thick plates.