As biodegradable thermoplastics are more and more penetrating the market of filaments for fused deposition modeling (FDM) 3D printing, fillers in the form of natural fibers are convenient: They have the clear advantage of reducing cost, yet retaining the filament biodegradability characteristics. In plastics that are processed through standard techniques (e.g., extrusion or injection molding), natural fibers have a mild reinforcing function, improving stiffness and strength, it is thus interesting to evaluate whether the same holds true also in the case of FDM produced components. The results analyzed in this review show that the mechanical properties of the most common materials, i.e., acrylonitrile-butadiene-styrene (ABS) and PLA, do not benefit from biofillers, while other less widely used polymers, such as the polyolefins, are found to become more performant. Much research has been devoted to studying the effect of additive formulation and processing parameters on the mechanical properties of biofilled 3D printed specimens. The results look promising due to the relevant number of articles published in this field in the last few years. This notwithstanding, not all aspects have been explored and more could potentially be obtained through modifications of the usual FDM techniques and the devices that have been used so far.
Despite the fact that wood polymer composites are interesting materials for many different reasons, they are quite difficult to shape through standard polymer processing techniques, such as extrusion or injection molding. Rheological characterization can be very helpful for understanding the role played by the many variables that are involved in manufacturing and to achieve a good quality final product through an optimized mix of formulation and processing parameters. The main methods that have been used for the rheological characterization of these materials are capillary and parallel plate rheometry. Both are very useful: rotational rheometry is particularly convenient to investigate the compounding phase and obtain structural information on the material, while capillary viscometry is well suited to understand final manufacturing. The results available in the literature at the moment are indeed very interesting and are mostly aimed at investigating the influence of the material formulation, the additives in particular, on the structural, mechanical, and morphological properties of the composite: despite a good number of papers, though, it is difficult to draw general conclusions, as many issues are still debated. The purpose of this article was to overview the state of the art and to highlight the issues that deserve further investigation.
Fused-filament fabrication is one of the most popular 3D printing techniques for thermoplastic materials because it is easy to use and is low-cost. On the other hand, it has the great limit of being suitable only for developing prototypes, because the printed object generally has low mechanical properties, and this prevents its use in structural applications. To solve this issue, the scientific literature has mainly focused on the optimization of the printing parameters and on performing some post-printing treatments, e.g., annealing, but despite some results being very promising, the topic has not yet been exhaustively investigated. In this paper, a post-printing treatment was studied that was based on two subsequent stages of remelting and compaction within a mold made of a granular material. The material chosen for this study was a green composite made of poly-(lactic acid) and poly-(hydroxyalkanoate) filled with wood fibers. The density, mechanical properties in terms of tension and microscopic observations were used to evaluate the treatment effectiveness. The main results were that voids were reduced, and the quality of the interlayer welding was increased, and this improved the mechanical properties, both in terms of stiffness and strength. In particular, the initial specimens displayed remarkable anisotropy, being stronger and stiffer in the longitudinal direction. After the post-processing treatment, despite the longitudinal properties having a very limited increase, the transversal properties increased significantly until they reached the longitudinal properties, thus leading to a more isotropic material.
In this study, the preparation of poly(vinyl alcohol) (PVA)/poly(lactic acid) (PLA) blends of different compositions, 100/0, 75/25, 50/50, 25/75, and 0/100, by mixing water solutions of the former and water dispersions of the latter polymer, is reported. Two distinct dispersions of PLA are prepared using a commercial‐grade polyester and two different surfactants, an anionic one and a neutral one. Films of PLA and of the corresponding blends are obtained by simply drying at 60 °C the water dispersions without or with the PVA. The films are characterized by infrared spectroscopy, differential scanning calorimetry (DSC), and scanning electron microscope (SEM) analysis. This evidences an island‐like morphology, with the continuous phase consisting of a PVA rich phase at all compositions except 25/75, for which an inverted phase composition, with a continuous phase made mostly of PLA, is instead found. Voids caused by air bubbles trapped in the initial mixture are observed in particular in the formulations with the anionic surfactant. The trapped bubbles result in premature thermal degradation by thermogravimetric analysis (TGA) and mechanical failure during clamping. Films with the neutral stabilizer are tougher than the bare commercial PLA, with Young modulus and elongation at break depending on the combination of the composition and arrangement of blend phases.
The use of wood fibers is a deeply investigated topic in current scientific research and one of their most common applications is as filler for thermoplastic polymers. The resulting material is a biocomposite, known as a Wood Polymer Composite (WPC). For increasing the sustainability and reducing the cost, it is convenient to increase the wood fiber content as much as possible, so that the polymeric fraction within the composite is thereby reduced. On the other hand, this is often thwarted by a sharp decrease in toughness and processability—a disadvantage that could be overcome by compounding the material with a toughening agent. This work deals with the mechanical properties in tension and impact of polypropylene filled with 50 wt.% wood flour, toughened with different amounts (0%, 10%, and 20%) of a polypropylene-based thermoplastic vulcanizate (TPV). Such properties are also investigated as a function of extrusion processing variables, such as the feeding mode (i.e., starve vs. flood feeding) and screw speed. It is found that the mechanical properties do depend on the processing conditions: the best properties are obtained either in starve feeding conditions, or in flood feeding conditions, but at a low screw speed. The toughening effect of TPV is significant when its content reaches 20 wt.%. For this percentage, the processing conditions are less relevant in governing the final properties of the composites in terms of the stiffness and strength.