ScF3 optical quality bulk crystals of the ReO3 structure type (space group , a = 4.01401(3) Å) have been grown from the melt by Bridgman technique, in fluorinating atmosphere for the first time. Aiming to substantially reduce vaporization losses during the growth process graphite crucibles were designed. The crystal quality, optical, mechanical, thermal and electrophysical properties were studied. Novel ScF3 crystals refer to the low-refractive-index (nD = 1.400(1)) optical materials with high transparency in the visible and IR spectral region up to 8.7 µm. The Vickers hardness of ScF3 (HV ~ 2.6 GPa) is substantially higher than that of CaF2 and LaF3 crystals. ScF3 crystals possess unique high thermal conductivity (k = 9.6 Wm−1К−1 at 300 K) and low ionic conductivity (σ = 4 × 10−8 Scm−1 at 673 К) cause to the structural defects in the fluorine sublattice.
A new scheme of two-beam X-ray diffractometry on the “X-Ray Crystallography and Physical Materials Science” (XCPM) beamline at the Kurchatov Synchrotron Radiation Source (KSRS) has been...
Molecular-beam epitaxial growth of Si-doped GaAs single-crystal layers on (110)-oriented GaAs substrates has been studied. The surface morphology of grown films was analyzed by scanning electron microscopy and atomic force microscopy, and the crystal structure of grown films was estimated by X-ray grazing incidence diffraction, in-plane pole figures, reciprocal space mapping, and photoluminescence spectroscopy. The type, concentration, and mobility of charge carriers in films were measured by the four-probe method in van der Pauw geometry at temperatures of 300 and 77 K. The possible existence of two areas in growth conditions, where increased concentration and mobility of electrons are achieved, was shown: the first, main area with the highest concentration and mobility values is Tg = 450–500 °C and V/III ratio γ = 20–40, the second, minor one is Tg = 600–680 °C and γ = 40–70. The hole conductivity was obtained at a growth temperature of 580 °C and a low γ value of 16. It was also shown that the defect-free crystal structure of the films grown at high temperatures is not necessarily accompanied by a smooth surface.