Increasing pollution of plastics smaller than 5 mm (microplastics [MPs]) in seas and oceans as well as in inland waters around the world has recently been a significant threat to water resources. In this study, MP pollution levels were investigated using a 335 µm mesh manta trawl in November 2019 in Van Bay. Water samples were collected from 15 stations. MP particles ranged from 641424 to 1426638 per km2 in surface waters (ranged from 2.35 to 5.09 MPs/m3 in water columns). The most frequently observed MP type, size, shape and colour classes were fiber (40.5%), <0.1 mm (52.3%), irregular (40.8%) and blue (57.1%), respectively. The highest MP abundance was observed at 14 and 15 stations where lake current were effective. Station 6 were also under serious plastic pollution pressure beacuse it was located close to Akkopru and Kurubas Rivers that pass through the densely populated city center. The chemical structure of all examined MPs showed presence of polyethylene (60.2%), followed by polypropylene (20.4%), polyethylene terephthalate (17.2%) and poly(methyl acrylate) (2.2%). The MPs were also examined using scanning electron microscopy to understand the surface characteristics. In conclusion, our study revealed that the surface waters of Van Bay are highly contaminated with MPs.
30 September 2019 in Bitlis Eren Üniversitesi Fen Bilimleri Dergisi
Bu çalışmada ilk kez sentezlenen p-tolil metil metakrilat polimerinin sentezi ve karakterizasyonu üzerinde çalışıldı. Bu amaçla sodyum metakrilatın p-totil klorürle reaksiyonundan p-tolil metil metakrilat monomeri sentezlendi. Monomer, başlatıcı olarak benzoil peroksit kullanılarak 60 oC’de serbest radikallik yolla polimerleştirildi. Elde edilen monomer ve polimerin yapısı IR, 1H-NMR, 13C-NMR teknikleriyle aydınlatıldı. Polimerin camsı geçiş sıcaklığı 65 oC, çözünürlük parametresi 8.69 (cal cm-3)1/2, GPS ile heterojenlik indisi 3.17 olarak bulundu. Bozunma sıcaklığı 205 oC ve yoğunluğu 1.12 gr cm-3 olarak belirlendi.
19 September 2025 in Polymer Engineering & Science
In this study, the effects of probe quantities on retention volume and the physical and thermodynamic results of polymer-probe systems were investigated. For this purpose, by using inverse gas chromatographic method. Alcohols and alkanes with different chemical and physical properties were injected as probes on homopolymer (2-cyclohexylidene-1,3-dioxolane-4-yl-methyl methacrylate) (CHMMA). Probe quantities of 0.3, 0.6, and 0.9 μl were selected, and an injection was made at every 10°C between 40 and 150°C. In addition, 3 μl volume probes were tried but reproducible results were not obtained in these volumes and the detector was observed to be out of order after several injections. It has been observed that the specific retention volume of alcohols and alkanes partially increased by increasing the injection amount. A linear relationship was observed between probe quantities and specific retention volume. This linear relationship is apparent from the specific retention volume values, where the probes are independent of the physical and chemical structures. It was observed that the results obtained in all three injections were close to each other and within acceptable limits. The glass transition temperature of the polymer was determined to be a of 60°C. The thermodynamic data calculated for the injection of different amounts of probes were close to each other.