Additive manufacturing (AM) techniques can be applied to produce carbon-fiber-reinforced polymer (CFRP) elements. Such elements can be exposed to different environmental factors, e.g., temperature, moisture, and UV radiation, related to their operational conditions. From a variety of environmental factors, the temperature is one of the most typical. Temperature strongly influences matrix material joining together CFRP components, resulting in material strength reduction. Therefore, it is important to understand processes in the composite material caused by temperature. This experimental work investigated the thermal effects on the performances of AM CFRP composites. Specimens with unidirectional (UD) alignments of the fiber reinforcement were printed using the fused deposition modeling (FDM) technique. The printed specimens were subjected to two different thermal conditions: stable continuous at 65 °C and cyclic temperature between 50 and 70 °C. Tensile testing was performed to study the mechanical strength and Young’s modulus of AM UD-CFRPs. In order to investigate the morphological structure on the surface of AM specimens, an optical microscope, scanning electron microscope (SEM), and digital microscope were utilized. Untreated (intact) samples attained the highest average tensile strength value of 226.14 MPa and Young’s modulus of 28.65 GPa. The ultimate tensile strength of the sample group subjected to stable heat treatment decreased to 217.99 MPa, while the thermal cycling group reduced to 204.41 MPa. The Young’s modulus of the sample group subjected to stable thermal exposure was decreased to 25.39 GPa, while for the thermal cycling group, it was reduced to 20.75 GPa. The visual investigations revealed that the intact or untreated specimen group exhibited lateral damage in top failure mode (LAT), the thermally stable group underwent edge delamination in the middle (DGM) as the nominated failure mode, and the explosive breakage at gauge in the middle (XGM) failure mode occurred in the sample from the thermal cycling group. Based on morphological observations at the microscale, the delamination, fiber pull-out, and matrix cracking were the dominant damages in the 3D-printed tensile-tested specimens. The molecular chains of the polymer changed their structure into an amorphous one, and only local motions of stretching occurred when the specimens were exposed to stable heating (prolonged). In the case of thermal cycling, the strain gradients were accumulated in the matrix material, and the local stresses increased as a result of the reheating and re-cooling exposure of the polymeric composites; the molecular motion of the long-range polymer structure was reactivated several times. Micro-cracking occurred as a result of internal stresses, which led to material failure and a reduction of the mechanical properties.
Additive manufacturing is a development of fabricating 3D parts layer by layer with complex geometries and utilized in numerous engineering structural applications. Fused deposition modeling technology provides higher design flexibility with aim of low cost and simplicity of material conversion to generate the composite parts. Previous studies have mainly focused on the manufacturing and characterization of continuous carbon fiber reinforced polymer composites (CCFRPCs) structure for fully dense and solid part structures and no study has been reported for porous CCFRPC parts. In this study, CCFRPCs porous structures were manufactured using FDM technology. The porous structures were fabricated with one perimeter shell by using two different types of infill patterns (grid and triangular) at three different infill densities levels (20%, 40%, and 60%). The reasons for developing such lightweight porous composite structures with continuous carbon fiber are the reduction of mass, efficient material utilization, energy consumption, and less waste generation. This study investigated the effects on tensile and flexural properties of composite specimens under uniaxial tensile loading and flexural loading, respectively. Fracture interface of the printed porous composites were examined and explored using optical microscope after performing mechanical tests. The experimental results demonstrated that infill pattern and density levels greatly affect the mechanical properties. The specimen printed using grid infill pattern with 60% infill density exhibited highest strength level in term of mechanical test and showed maximum tensile and flexural strength of 162.9 MPa and 127.24 MPa, respectively. While triangular infill pattern with 60% infill density level revealed the maximum tensile and flexural strength of 152.62 MPa and 117.53 MPa, respectively. Hence, from the results achieved in this study showed great potential and ability to replace fully dense and solid structure by the porous structure.
Polytetrafluoroethylene (PTFE) was coated on 316L stainless steel (SS) substrate through a spin coating technique to enhance its corrosion resistance properties in hydrochloric acid (HCl) and nitric acid (HNO3) medium. Scanning electron microscopy (SEM) revealed the morphology of the coated and uncoated substrates and showed a uniform and crack-free PTFE coating on 316L SS substrate, while a damaged surface with thick corrosive layers was observed after the electrochemical test on the uncoated sample. However, an increased concentration of HCl and HNO3 slightly affected the surface morphology by covering the corrosive pits. An atomic force microscope (AFM) showed that the average surface roughness on 316L SS and PTFE coating was 26.3 nm and 24.1 nm, respectively. Energy dispersive X-ray spectroscopy (EDS) was used for the compositional analysis, which confirmed the presence of PTFE coating. The micro Vickers hardness test was used to estimate the hardness of 316L SS and PTFE-coated substrate, while the scratch test was used to study the adhesion properties of PTFE coating on 316L SS. The anticorrosion measurements of 316L SS and PTFE-coated substrates were made in various HCl and HNO3 solutions by using the electrochemical corrosion test. A comparison of the corrosion performance of PTFE-coated substrate with that of bare 316L SS substrate in HCl medium showed a protection efficiency (PE) of 96.7%, and in the case of HNO3 medium, the PE was 99.02%, by slightly shifting the corrosion potential of the coated sample towards the anodic direction.