The effect of the scanning strategy during selective laser melting (SLM) of Ti-6Al-4V was investigated. An optimized cellular scan strategy (island scan modeled) was compared to a simple cellular scan strategy (island scan stripes) and a simple antiparallel line scanning strategy (line scan). Surface texture was investigated by optical three-dimensional (3D) surface measurements, which when combined with light optical microscopy (LOM), revealed deflections caused by the thermal stresses during the build process. Elevated edges caused by the edge-effect dominate the surface texture of all investigated specimens. The scanning strategy determines the surface texture, and the lowest surface roughness was obtained by the line scan strategy. Porosity was investigated with X-ray computed tomography-imaging. Mainly spherical porosity was observed for the line scan and island scan modeled specimens, while the island scan stripes strategy showed more lack-of-fusion defects and a higher total porosity amount. Microstructure was investigated with LOM and scanning electron microscopy (SEM). The microstructure in Ti-6Al-4V was largely martensitic α’ and prior β grains. The morphology is different for the various scan strategies, and decomposition of α’ into lamellar α/β was observed in the bottom part of the island scan specimen. Accordingly, the hardness decreased in the decomposed part of the specimen.
1 February 2020 in Surface and Coatings Technology
Wire arc additive manufacturing (WAAM) direct energy deposition is used to process two different Duplex Stainless-Steels (DSS) wire chemistries. Macro and micro mechanical response variables relevant to industrialization are studied using a Design of the Experiment (DoE) approach.The tested window of operation (i.e., 0.09 kJ/mm ≥ Heat Input (HI) ≥ 0.23 kJ/mm – nominal value) show that variation of layer height and overthickness are highly correlated with travel speed and wire feed speed and positively correlated with heat input. The maximum achieved average instantaneous deposition rate is 3.54 kg/h. Besides, the wire chemistry G2205, with a decreased nickel content, shows a stable ferrite-to-austenite ratio of equal proportions (i.e., Fe% = 49.20 ± 1.92 % and HV3 = 252.8 ± 3.55), whereas G2209 provides a reduced ferrite content (i.e., Fe% = 29.69 ± 0.56 % and HV3 = 241.6 ± 3.17). Part geometry and weaving strategy affect the homogeneous distribution of Fe% distribution and high heat inputs lead to coarser microstructures with dendritic morphology.The manufacturing weaving strategy creates local heterogeneous microstructure with varying Fe%. Thus, an understanding of this effect with higher-dimensional design spaces, uncertainty quantification, and dynamic process control are required to drive metal WAAM towards full industrialization.