In this study, wear resistance and some selected physical properties of pawpaw–glass fiber hybrid reinforced epoxy composites were investigated. Two different layers of pawpaw stem—linear and network structures—were extracted and chemically modified. Hybrid reinforced composites were developed comparatively from the two fiber structures and glass fiber using hand lay-up in an open mold production process. The wear resistance was studied via the use of a Taber Abrasion Tester while selected physical properties were also investigated. The influence of the fiber structure on the properties examined revealed that network structured pawpaw fiber was the best as reinforcement compared to the linearly structured fiber. The addition of these vegetable fibers to epoxy resin brought about improved thermal conductivity and increased the curing rate while the wear resistance of the corresponding developed composites were enhanced by 3 wt% and 15 wt% of fibers from linear and network pawpaw fibers. It was noticed that linearly structured pawpaw fiber had its best result at 3 wt% while network structured pawpaw fiber had its best result at 15 wt%.
This study investigates the development of lightweight, hybrid reinforced epoxy composites using chicken feather fiber (CFF) and glass fiber (GF) as reinforcements for automotive applications. The composites were fabricated by combining treated chicken feather fibers and glass fibers in a 1:1 wt ratio within an epoxy matrix. The mechanical, thermal, and abrasion properties of the composites were assessed through tensile, flexural, hardness, impact, and wear tests, alongside thermal conductivity measurements. The results revealed that the tensile strength (62.49 MPa) and modulus (801.28 MPa) peaked at 12 wt% reinforcement, with increases of 54% and 36%, respectively, compared to the unreinforced epoxy. The composite with 9 wt% hybrid reinforcement exhibited the highest flexural strength (119.37 MPa), while the 12 wt% hybrid composites showed the best impact resistance (27.9 J/mm 2 ). The wear resistance showed that all the reinforced composites had improved wear resistance, with 18 wt% having the highest wear resistance of 0.12 mg. Additionally, the reinforced composites demonstrated lower thermal conductivity with increasing fiber content as compared with the unreinforced composite, with 12 wt% reinforcement having the lowest thermal conductivity value of 0.000018 W/mK. SEM analysis revealed a strong interfacial bonding between the fibers and the matrix, contributing to the composites’ improved mechanical and thermal properties. The successful hybridization of chicken feathers and glass fibers offers a promising sustainable approach for structural and environmental applications such as automotive components, providing lightweight materials with improved performance, cost-effectiveness, and environmental benefits over traditional materials.