Djarot Darmadi

Dr. Djarot Darmadi


Research Focus & Metrics

Academic Career Length

11Years (2016-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
24 January 2023 in International Journal of Hydrogen Energy
Verified
Journal Article
Closed access
FGFemiana Gapsari
Femiana Gapsari
DDDjarot Darmadi
Djarot Darmadi
PSPutu H. Setyarini
Putu H. Setyarini
HWHastono Wijaya
Hastono Wijaya
KMKartika A. Madurani
Kartika A. Madurani
HHHendra Hermawan
Hendra Hermawan

3 November 2021 in Sustainability
Verified
Journal Article
Open access
PDF file
FGFemiana Gapsari
Femiana Gapsari
DDDjarot Darmadi
Djarot Darmadi
PSPutu H. Setyarini
Putu H. Setyarini
HIHubby Izzuddin
Hubby Izzuddin
KMKartika A. Madurani
Kartika A. Madurani
HHHendra Hermawan
Hendra Hermawan
Organic inhibitors have been considered as an effective way to control the corrosion of carbon steel weldment in an acidic environment. This work proposes a new green organic inhibitor made of extract of rambutan fruit (Nephelium lappaceum) peel and aims at analyzing its corrosion inhibitor properties and protection mechanism. Specimens of carbon steel weldment were tested for their corrosion by using electrochemical and immersion methods in 1 M HCl solution containing 0 to 6 g/L of Nephelium peel (NP) extract. Results showed that, in the same solution, the corrosion rate was measured to be higher on the weld metal zone than that of base metal zone, which could be related to the coarser grain of the weld metal zone and the stability of the formed oxide layer. The addition of NP extract was found to increase the stability of the oxide layer, thus increasing the corrosion resistance of the specimens. The maximum inhibition efficiency of the NP extract was reached at 97% for weld metal with 5 g/L of extract, at 80% for the heat affected zone with 5 g/L, and at 70% for base metal with 4 g/L. This work reveals the particularity of different weldment zones to the different needs of inhibitor concentration for obtaining the optimum corrosion protection.

9 February 2024 in Heliyon
Verified
Journal Article
Open access
TWTeguh Widjajanto
Teguh Widjajanto
DDDjarot Darmadi
Djarot Darmadi
YIYudy Surya Irawan
Yudy Surya Irawan
FGFemiana Gapsari
Femiana Gapsari
Circulating Fluidized Bed (CFB) boiler often experience leaks in the wall tube due to corrosion and abrasion of the bed material after use that varies between 3 and 8 months. To avoid erosion corrosion, a coating was done in the form of Chrome Clad Tube Armor (CTA). In this research, a Failure Analysis (FA) was performed on the characterization of the boiler tube using several types of samples, which are Wall Tube Without Coating (WT) and CTA (in new condition and after eight months of use). Macro visual, Field emission scanning electron microscopes (FE-SEM), Fourier-transform infrared spectroscopy (FTIR), corrosion, and Thermogravimetric analysis (TGA) tests showed that the CTA type has better corrosion and thermal resistance. The hardness values of the CTA and WT coating substrates after eight months of use were 197.75 and 195.2 HV. The failure mechanism on the tube was caused by high temperatures (long-term overheating) and friction between the tube and the fluid or metal. Wall tubes in furnaces fail due to erosion and corrosion due to fluid and solid particle mixtures and environmental contact.

16 February 2022 in Case Studies in Thermal Engineering
Verified
Journal Article
Open access
NTNurdin Hasananto Teguh
Nurdin Hasananto Teguh
LYLilis Yuliati
Lilis Yuliati
DDDjarot Darmadi
Djarot Darmadi

31 December 2022 in Salud, Ciencia y Tecnología
Verified
Journal Article
Open access
PDF file
RBRedi Bintarto
Redi Bintarto
APAnindhito Purnowidodo
Anindhito Purnowidodo
DDDjarot Darmadi
Djarot Darmadi
TWTeguh Dwi Widodo
Teguh Dwi Widodo
The increasingly widespread use of galvanized roofs certainly has an effect on the occupants in the room below. Among them is a hot room temperature. For that reason, it is necessary to make new discoveries in the field of composites of natural materials to overcome them because most natural materials, especially natural stone, have low thermal conductivity, which means they can inhibit heat propagation. This study sought to ascertain how much andesite natural stone powder, combined with epoxy, can lower the room temperature when it is layered on a galvanized roof. Different amounts of natural stone powder applied to a galvanized roof results in different thermal conductivities. The temperature readings were taken at a height of 20 cm above the roof, right at the bottom galvanic, as well as the temperature in the room below. Our results showed that adding andesite natural stone powder to the roof was able to lower the room temperature, and the thicker the composite layer in coating the galvanized roof, the lower the room temperature under the roof

23 March 2020 in Applied Sciences
Verified
Journal Article
Open access
PDF file
DDDjarot Darmadi
Djarot Darmadi
FGFemiana Gapsari
Femiana Gapsari
Osmar LoboOsmar Lobo
Osmar Lobo
Firman mangasa SimanjuntakFirman mangasa Simanjuntak
Firman mangasa Simanjuntak
Stress corrosion cracking (SCC) is known as a major factor that should be considered in the assessment of welding joint structure integrity. Despite the promising and wide application of dissimilar metal joints, the currently available SCC mitigation technique of dissimilar metal joints is not adequate. The challenge is to obtain a good joint while different melting points exist. This article reports a novel SCC mitigation method on a brass–steel dissimilar metal joint by modifying the geometry of the surface. It is evidenced that the sharpened steel (α1 specimen) significantly improves the SCC resilience of the joint. The evaluation of SEM/EDS photos reveals that the α1 geometry induces a smaller pore area around brass–steel micro-joint interfaces which in turn produces stronger joints.