15 June 2009 in Journal of Applied Physics
Verified
Journal Article
Closed access
PDF file
TTT. Teraji
T. Teraji
YGYiuri GARINO
Yiuri GARINO
YKY. Koide
Y. Koide
TIT. Ito
T. Ito
Room-temperature fabrication of Schottky diodes was demonstrated for p -type boron-doped diamond. This fabrication method’s key technique is selective modification of surface termination from monohydride into oxygen groups using vacuum ultraviolet light irradiation in oxygen. The Au contacts, formed on the hydrogen-terminated surface, maintained Ohmic properties after this selective surface oxidation. The Au contacts then deposited on the oxidized surface, imparting Schottky properties. The lateral-type diodes comprising Au Schottky contacts and Au Ohmic contacts showed blocking voltage higher than 1 kV without electrode guarding. The leakage current at 1 kV was as low as 30 pA.

1 October 2019 in Spectrochimica Acta Part B: Atomic Spectroscopy
Verified
Journal Article
Closed access
AFA. Fau
A. Fau
OBO. Beyssac
O. Beyssac
MGM. Gauthier
M. Gauthier
PMP.Y. Meslin
P.Y. Meslin
ACA. Cousin
A. Cousin
SMS. Maurice
S. Maurice

1 April 2006 in Diamond and Related Materials
Verified
Journal Article
Closed access
ABA. Balducci
A. Balducci
YGYiuri GARINO
Yiuri GARINO
AGAlessandro Lo Giudice
Alessandro Lo Giudice
CMC. Manfredotti
C. Manfredotti
MMMarco Marinelli
Marco Marinelli
GRGianluca Verona Rinati
Gianluca Verona Rinati

10 April 2006 in Applied Physics Letters
Verified
Journal Article
Closed access
PDF file
YGYiuri GARINO
Yiuri GARINO
AGAlessandro Lo Giudice
Alessandro Lo Giudice
CMC. Manfredotti
C. Manfredotti
MMMarco Marinelli
Marco Marinelli
EME. Milani
E. Milani
GRGianluca Verona Rinati
Gianluca Verona Rinati
Pulsed x-ray dose measurements have been carried at maximum x-ray energies from 40to120KeV out by using a single crystal epitaxial diamond sample grown by chemical vapor deposition (CVD). Delivered doses were between 0.1 and 10mGy and pulse duration times between 0.01 and 0.5s . Values of dose linearity index very close to 1 (between 1.02 and 1.07) at increasing x-ray energies and pulse decay times between 15 and 20ms were obtained. The reproducibility was very good with no memory effects. CVD homoepitaxial diamond results to be very promising for x-ray diagnostic applications.

9 September 2009 in Physica Status Solidi (a)
Verified
Journal Article
Closed access
PDF file
YGYiuri GARINO
Yiuri GARINO
OTOkuyuki Teraji
Okuyuki Teraji
SKSatoshi Koizumi
Satoshi Koizumi
YKYasuo Koide
Yasuo Koide
TIToshimichi Ito
Toshimichi Ito

12 November 2018 in Physical Review B
Verified
Journal Article
Closed access
PDF file
FDFrédéric Decremps
Frédéric Decremps
SASimon Ayrinhac
Simon Ayrinhac
MGMichel Gauthier
Michel Gauthier
DADaniele Antonangeli
Daniele Antonangeli
MMMarc Morand
Marc Morand
PPParaskevas Parisiades
Paraskevas Parisiades
Liquid cesium (l-Cs) sound velocity at high densities was investigated along a 500-K isotherm using high-pressure picosecond acoustics measurements. At 2.0 GPa, the liquid sound velocity goes through a maximum versus pressure without any change on the reflectivity and interferometry acoustic signals. Upon further compression, a softening of the l-Cs viscoelastic properties is observed from 2.0 up to 4.0 GPa, pressure at which the reflectometric signal is abruptly reversed whereas the interferometric signal remains qualitatively the same. This anomalous behavior could be related to an electronic transformation within the l-Cs state, which here again could reflect what happens at lower temperature within the solid state. If so, such liquid-liquid transition may be driven by the progressive collapse of the 6s electronic orbital onto the 5d ones. Above 4.0 GPa, the l-Cs sound velocity starts again to increase as commonly expected upon compression.