In circular economy, useful plastic materials are kept in circulation as opposed to being landfilled, incinerated, or leaked into the natural environment. Pyrolysis is a chemical recycling technique useful for unrecyclable plastic wastes that produce gas, liquid (oil), and solid (char) products. Although the pyrolysis technique has been extensively studied and there are several installations applying it on the industrial scale, no commercial applications for the solid product have been found yet. In this scenario, the use of plastic-based char for the biogas upgrading may be a sustainable way to transform the solid product of pyrolysis into a particularly beneficial material. This paper reviews the preparation and main parameters of the processes affecting the final textural properties of the plastic-based activated carbons. Moreover, the application of those materials for the CO2 capture in the processes of biogas upgrading is largely discussed.
This work focuses on the use of a char produced during the pyrolysis of a mixture of non-recyclable plastics as a precursor for the preparation of porous activated carbon with high developed adsorption uptake of lead in water. Physical and chemical activation was used to enhance the porosity, surface area, and surface chemistry of char. The final activated carbon materials were deeply characterized through N2 adsorption isotherms, scanning electron microscopy, Fourier transformed infrared spectroscopy, analysis of the metal content by inductively coupled plasma mass spectroscopy, and pH of point zero charge. The native char displayed a Pb adsorption uptake of 348 mg Pb·g−1 and considerably high leaching of carbon, mainly organic, ca. 12%. After stabilization with HCl washing and activation with basic character activators, i.e., CO2, NaOH, and KOH, more stable adsorbents were obtained, with no organic leaching and a porous developed structure, the order of activation effectiveness being KOH (487 m2·g−1) > NaOH (247 m2·g−1) > CO2 (68 m2·g−1). The activation with KOH resulted in the most effective removal of Pb in water with a saturation adsorption uptake of 747 mg Pb·g−1.