The photon absorption in Si quantum dots (QDs) embedded in SiO2 has been systematically investigated by varying several parameters of the QD synthesis. Plasma-enhanced chemical vapor deposition (PECVD) or magnetron cosputtering (MS) have been used to deposit, upon quartz substrates, single layer, or multilayer structures of Si-rich-SiO2 (SRO) with different Si content (43–46 at. %). SRO samples have been annealed for 1 h in the 450–1250 °C range and characterized by optical absorption measurements, photoluminescence analysis, Rutherford backscattering spectrometry and x-ray Photoelectron Spectroscopy. After annealing up to 900 °C SRO films grown by MS show a higher absorption coefficient and a lower optical bandgap (∼2.0 eV) in comparison with that of PECVD samples, due to the lower density of Si–Si bonds and to the presence of nitrogen in PECVD materials. By increasing the Si content a reduction in the optical bandgap has been recorded, pointing out the role of Si–Si bonds density in the absorption process in small amorphous Si QDs. Both the photon absorption probability and energy threshold in amorphous Si QDs are higher than in bulk amorphous Si, evidencing a quantum confinement effect. For temperatures higher than 900 °C both the materials show an increase in the optical bandgap due to the amorphous-crystalline transition of the Si QDs. Fixed the SRO stoichiometry, no difference in the optical bandgap trend of multilayer or single layer structures is evidenced. These data can be profitably used to better implement Si QDs for future PV technologies.
In this work the Si self-interstitial–carbon interaction has been experimentally investigated and modeled. The interactions between self-interstitials, produced by 20-keV silicon implantation, and substitutional carbon in silicon have been studied using a layer grown by molecular beam epitaxy (MBE) and interposed between the near-surface self-interstitial source and a deeper B spike used as a marker for the Si-interstitial concentration. The C atoms, all incorporated in substitutional sites and with a C-dose range of trap the self-interstitials in such a manner that the layer behaves as a filtering membrane for the interstitials flowing towards the bulk and, consequently, strongly reduces the boron-enhanced diffusion. This trapping ability is related to the total C dose in the membrane. Substitutional carbon atoms interacting with self-interstitials are shown to trap Si interstitials, to be removed from their substitutional sites, and to precipitate into the C-rich region. After precipitation, C atoms are not able to further trap injected self-interstitials, and the interstitials generated in the surface region can freely pass through the C-rich region and produce B-enhanced diffusion. The atomistic mechanism leading to Si-interstitial trapping has been investigated by developing a simulation code describing the migration of injected interstitials. The simulation takes into account the surface recombination, the interstitial diffusion in our MBE-grown material, and C traps. Since the model calculates the amount of interstitials that actually react with C atoms, by a comparison with the experimental data it is possible to derive quantitative indications of the trapping mechanism. It is shown that one Si interstitial is able to deactivate about two C traps by means of interstitial trapping and C clustering reactions. The reaction causing trapping and deactivation is tentatively described.
Determination of the optical bandgap (Eg) in semiconductor nanostructures is a key issue in understanding the extent of quantum confinement effects (QCE) on electronic properties and it usually involves some analytical approximation in experimental data reduction and modeling of the light absorption processes. Here, we compare some of the analytical procedures frequently used to evaluate the optical bandgap from reflectance (R) and transmittance (T) spectra. Ge quantum wells and quantum dots embedded in SiO2 were produced by plasma enhanced chemical vapor deposition, and light absorption was characterized by UV-Vis/NIR spectrophotometry. R&T elaboration to extract the absorption spectra was conducted by two approximated methods (single or double pass approximation, single pass analysis, and double pass analysis, respectively) followed by Eg evaluation through linear fit of Tauc or Cody plots. Direct fitting of R&T spectra through a Tauc-Lorentz oscillator model is used as comparison. Methods and data are discussed also in terms of the light absorption process in the presence of QCE. The reported data show that, despite the approximation, the DPA approach joined with Tauc plot gives reliable results, with clear advantages in terms of computational efforts and understanding of QCE.
We present extended x-ray absorption fine structure (EXAFS) analyses of the Er edge in Er-doped (100) Si samples. The samples were prepared by multiple implants of Er and O resulting in the incorporation of Er/cm and O/cm in a 2.3- m-thick amorphous layer. It has been found that the local environment around the Er sites, which consists of six Si first neighbors in the amorphous layer, evolves towards a mixed coordination with O and Si atoms after epitaxial regrowth of the layer at C for 3 h. A further thermal treatment at C removes the residual Er–Si coordination and produces a full oxygen coordinated first shell with an average of 5 O neighbors. The effects of the different thermal processes on the high resolution spectra of the 1.54 m Er photoluminescence were also measured and related to the EXAFS results.
Visible luminescence from ZnO nanorods (NRs) is attracting large scientific interest for light emission and sensing applications. We study visible luminescent defects in ZnO NRs as a function of post growth thermal treatments, and find four distinct visible deep level defect states (VDLSs): blue (2.52 eV), green (2.23 eV), orange (2.03 eV), and red (1.92 eV). Photoluminescence (PL) studies reveal a distinct modification in the UV (3.25 eV) emission intensity and a shift in the visible spectra after annealing. Annealing at 600 °C in Ar (Ar600) and O2 (O600) causes a blue and red-shift in the visible emission band, respectively. All samples demonstrate orange emission from the core of the NR, with an additional surface related green, blue, and red emission in the As-Prep, Ar600, and O600 samples, respectively. From PL excitation (PLE) measurements we determine the onset energy for population of the various VDLSs, and relate it to the presence of an Urbach tail below the conduction band due to a presence of ionized Zni or Zni complexes. We measured an onset energy of 3.25 eV for the as prepared sample. The onset energy red-shifts in the annealed samples by about 0.05 to 0.1 eV indicating a change in the defect structure, which we relate to the shift in the visible emission. We then used X-ray photoemission spectroscopy (XPS), and elastic recoil detection analysis (ERDA) to understand changes in the surface structure, and H content, respectively. The results of the XPS and ERDA analysis explain how the chemical states are modified due to annealing. We summarize our results by correlating our VDLSs with specific intrinsic defect states to build a model for PL emission in ZnO NRs. These results are important for understanding how to control defect related visible emission for sensing and electroluminescence applications.