Assim Lateef

Dr. Assim Lateef

orcid

Research Focus & Metrics

Academic Career Length

6Years (2021-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
11 August 2023 in Tikrit Journal of Engineering Sciences
Verified
Journal Article
Open access
PDF file
AAAdnan Ibrahim Abdullah
Adnan Ibrahim Abdullah
ALAssim Lateef
Assim Lateef
External strengthening of reinforced-concrete beams is challenging because of the building system complexity or the beam geometry. The major challenge is choosing an appropriate strengthening method to overcome its low torsion strength. Therefore, the main objective of this research is to ascertain how likely it is to suggest or adopt a particular internal in-plane approach to increase the torsional strength. In the present paper, the concept (technique) of adding internal concrete cross-rods (CR) in a transverse direction is adopted. Five concrete beam specimens with 200-, 200-, and 1500-mm dimensions for width, depth, and length, respectively, were poured and tested. One was a reference beam(B-R) without enhancement, while the other four (B-3CR, B-5CR, B-7CR, and B-9CR) were enhanced with three, five, seven, and nine internal cross-rod, respectively. The compressive strength of the concrete was (35MPa) at (28) days (normal strength concrete). This research intends to show how internal cross-rods (CR) and their number affect torsional capability. The experimental findings revealed significant improvements in the ultimate torsion strength capability by about 11.65%, 18.95%, 21.24%, and 27.77%, respectively, compared to the reference beam. The ultimate twisting angle and reinforced beams’ toughness increased by (4.25%-28.36%) and (24.12%-94.48%), respectively, due to the increase in the number of internal cross-rods compared to the reference beam. It was concluded that interior cross-rods would enhance the torsional strength capacity of the reinforced concrete beams. The extent of enhancement depended mainly on the number of internal cross-rods (CR) deployed.

20 August 2024 in Innovative Infrastructure Solutions
Verified
Journal Article
Closed access
PDF file
RIRuqaya K Ibrahim
Ruqaya K Ibrahim
ALAssim Lateef
Assim Lateef

15 July 2021 in Tikrit Journal of Engineering Sciences
Verified
Journal Article
Open access
AAAbd-Al-Salam I. M. Al-Hazragi
Abd-Al-Salam I. M. Al-Hazragi
ALAssim Lateef
Assim Lateef
This article investigates the behaviour of strengthened concrete columns using jacketing ultra-high-performance fiber reinforced concrete (UHPFRC) and carbon fiber-reinforced polymer (CFRP) under uniaxial loaded. The jacket was connected to the column core using shear connectors and (CFRP) fixed as a strip on the tension zone between the column cores and the jacketing. Seven column samples of square cross-section (120 x120) mm at the midsection with overall length of 1250 mm were cast using normal strength concrete (NSC) and having similar longitudinal and transverse reinforcement. The samples were made and tested under axial load at eccentricity equal to 120 mm up to failure. Test parameters were the thickness of jackets (25 and 35) mm and the width of CFRP (0,8, and 12) cm. Column specimens were tested, one of them was reference without any strengthening, and the other specimens divided into two groups (A, and B), and each group included three specimens based on the parameters. Group (A) has UHPFRC jacket thickness 25 mm and CFRP width (0,8, and 12) cm respectively, and group (B) has UHPFRC jacket thickness 35 mm and CFRP width (0,8, and 12) cm respectively. The outcomes of the article show that increasing the thickness of jacket, and width of CFRP lead to increase in the load carrying capacity about (110.5%,168.4%, and 184.2%) for group A, and (157.9%,226.3%, and 263.2%) for group B compared with the reference column due to delay in the appearance of cracks and their distribution. The mid-height lateral displacement of columns was decreased about (66.6%,42.3%, and 35.9%) for group A, and (46.15%,38.46%, and 32.3%) for group B, also the axial deformation of specimens decreased about (71.7%,60.86%, and 55.86%) for group A, and (65.5%,60.5%, and 53.4) for group B compared with the reference column. The ductility of columns that were strengthened with UHPFRC jacket only was increased about (13.67%,19.66%) for thickness(25,35) mm respectively, because of that UHPFRC jacket was contented on steel fibers, and the percentage decrease of ductility was about (5.1%,and 12%) for group (A), (1%,and 9.4%) for group (B) when bonded CFRP in the tension zone with width (8 ,and 12) cm respectively. The results show improvement in the initial and secant stiffness when, increased the thickness of jacket, and width of CFRP because of increase in the size of columns and improvement in the modulus of elasticity. The toughness increase was about (273.97%,301.55%, and 304.5%) for group A, and (453.69%,511.93%, and 524.28%) for group B compared with the reference column because of increase in the size of specimens and delay the appearance of cracks.

8 October 2024 in Tikrit Journal of Engineering Sciences
Verified
Journal Article
Open access
PDF file
SMSufyan E. Mutlag
Sufyan E. Mutlag
ALAssim Lateef
Assim Lateef
The torsional behavior of twelve concrete-filled steel tube (CFST) specimens was experimentally investigated. CFST specimens were reinforced by internal cross-rods with different spacing (0, 50, 100, 150, 200, and 250) mm, different thicknesses of the steel tube (1.5 and 2) mm, and a compressive strength of 65 MPa (high strength concrete). Each sample was tested, and the results were examined. According to the results, the infill concrete prevented buckling failure in CFST specimens. The steel tube and concrete worked together since cutting steel tubes caused diagonal cracks in the infill concrete of CFST specimens. The results also showed that the CFST's torsional moment capacity increased due to the concrete infill, further aiding the steel tubes' performance. Internal stiffening in the steel tubes and concrete infill improved the failure mode, mechanical properties, and CFST specimens’ behavior under torsion.

22 August 2025 in Infrastructures
Verified
Journal Article
Open access
PDF file
SHSWAR IMAD HASIB
SWAR IMAD HASIB
ALAssim Lateef
Assim Lateef
OAOmar Warani Aziz
Omar Warani Aziz
The main objective of this research is to investigate the impact of the tendon profile layout on the shear strength of unbonded post-tensioned prestressed concrete bridge I-girders. This study involves an experimental investigation where ten unbonded post-tensioned bridge girders are cast and subjected to four-point loads. The focus of the investigation is on the effect of different tendon profile layouts, including trapezoidal, parabolic, and harped shapes. The experimental results reveal that the shear behavior of the specimens progresses through three distinct stages: the elastic stage, the elastic–plastic stage, and the plastic stage, with all specimens ultimately failing due to shear. The results show that tendon profiles with higher eccentricity at the end of the beams (80 mm above the neutral axis) had the highest ultimate load capacity for each tendon profile shape, coupled with the largest deflection. Conversely, profiles with lower eccentricity (80 mm below the neutral axis) demonstrated the lower ultimate load capacity for each tendon profile shape and minimal deflection. Among the various tendon profile layouts that were tested, the specimen with the harped tendon profile (GF-1 HA) showed the highest ultimate load capacity, with an increasing rate of 17.52% in ultimate load and a 45.55% increase in ultimate deflection compared to the control beam (GF-1 ST) with a straight tendon profile. On the other hand, the harped tendon profile specimen (GF-1 HA) exhibited the lowest deflection among the various tendon profile shapes with an increasing rate of 5.7% in ultimate load deflection in comparison with the control beam (GF-1 ST) with a straight tendon profile. These improvements in stiffness, load capacity, and deflection are attributed to enhanced resistance, particularly at the supports. Consequently, the optimized tendon layouts offer an increase in the overall structural efficiency, leading to potential cost savings in bridge girder production.

20 March 2021 in Tikrit Journal of Engineering Sciences
Verified
Journal Article
Open access
AAAbd-Al-Salam Al-Hazragi
Abd-Al-Salam Al-Hazragi
ALAssim Lateef
Assim Lateef
This article investigates the behaviour of strengthened concrete columns using jacketing ultra-high-performance fiber reinforced concrete (UHPFRC) and carbon fiber-reinforced polymer (CFRP) under uniaxial loaded. The jacket was connected to the column core using shear connectors and (CFRP) fixed as a strip on the tension zone between the column cores and the jacketing. Seven column samples of square cross-section (120 x120) mm at the midsection with overall length of 1250 mm were cast using normal strength concrete (NSC) and having similar longitudinal and transverse reinforcement. The samples were made and tested under axial load at eccentricity equal to 120 mm up to failure. Test parameters were the thickness of jackets (25 and 35) mm and the width of CFRP (0,8, and 12) cm. Column specimens were tested, one of them was reference without any strengthening, and the other specimens divided into two groups (A, and B), and each group included three specimens based on the parameters. Group (A) has UHPFRC jacket thickness 25 mm and CFRP width (0,8, and 12) cm respectively, and group (B) has UHPFRC jacket thickness 35 mm and CFRP width (0,8, and 12) cm respectively. The outcomes of the article show that increasing the thickness of jacket, and width of CFRP lead to increase in the load carrying capacity about (110.5%,168.4%, and 184.2%) for group A, and (157.9%,226.3%, and 263.2%) for group B compared with the reference column due to delay in the appearance of cracks and their distribution. The mid-height lateral displacement of columns was decreased about (66.6%,42.3%, and 35.9%) for group A, and (46.15%,38.46%, and 32.3%) for group B, also the axial deformation of specimens decreased about (71.7%,60.86%, and 55.86%) for group A, and (65.5%,60.5%, and 53.4) for group B compared with the reference column. The ductility of columns that were strengthened with UHPFRC jacket only was increased about (13.67%,19.66%) for thickness(25,35) mm respectively, because of that UHPFRC jacket was contented on steel fibers, and the percentage decrease of ductility was about (5.1%,and 12%) for group (A), (1%,and 9.4%) for group (B) when bonded CFRP in the tension zone with width (8 ,and 12) cm respectively. The results show improvement in the initial and secant stiffness when, increased the thickness of jacket, and width of CFRP because of increase in the size of columns and improvement in the modulus of elasticity. The toughness increase was about (273.97%,301.55%, and 304.5%) for group A, and (453.69%,511.93%, and 524.28%) for group B compared with the reference column because of increase in the size of specimens and delay the appearance of cracks.