Recently, research into the factors that influence the formation and growth of intermetallic compounds (IMCs) layer in lead-free solders has piqued interest, as IMCs play an important role in solder joints. The reliability of solder joints is critical to the long-term performance of electronic products. One of the most important factors which are known to influence solder joint reliability is the intermetallic compound (IMC) layer formed between the solder and the substrate. Although the formation of an IMC layer signifies good bonding between the solder and substrate, its main disadvantage is due to its brittle nature. This paper reviews the formation and growth of IMCs in lead-free solder joints detailing the effect of alloying additions, surface finishes, aging time, aging temperature and solder volume. The formation and growth of the brittle IMCs were significantly affected by these factors and could be possibly controlled. This review may be used as a basis in understanding the major factors effecting the IMC formation and growth and relating it to the reliability of solder joints.
Geopolymer materials are used as construction materials due to their lower carbon dioxide (CO2) emissions compared with conventional cementitious materials. An example of a geopolymer material is alkali-activated kaolin, which is a viable alternative for producing high-strength ceramics. Producing high-performing kaolin ceramics using the conventional method requires a high processing temperature (over 1200 °C). However, properties such as pore size and distribution are affected at high sintering temperatures. Therefore, knowledge regarding the sintering process and related pore structures on alkali-activated kaolin geopolymer ceramic is crucial for optimizing the properties of the aforementioned materials. Pore size was analyzed using neutron tomography, while pore distribution was observed using synchrotron micro-XRF. This study elucidated the pore structure of alkali-activated kaolin at various sintering temperatures. The experiments showed the presence of open pores and closed pores in alkali-activated kaolin geopolymer ceramic samples. The distributions of the main elements within the geopolymer ceramic edifice were found with Si and Al maps, allowing for the identification of the kaolin geopolymer. The results also confirmed that increasing the sintering temperature to 1100 °C resulted in the alkali-activated kaolin geopolymer ceramic samples having large pores, with an average size of ~80 µm3 and a layered porosity distribution.
This paper elucidates the effect of isothermal ageing at temperature of 85 °C, 125 °C and 150 °C for 100, 500 and 1000 h on Sn-3.0Ag-0.5Cu (SAC305) lead-free solder with the addition of 1 wt% kaolin geopolymer ceramic (KGC) reinforcement particles. SAC305-KGC composite solders were fabricated through powder metallurgy using a hybrid microwave sintering method and reflowed on copper substrate printed circuit board with an organic solderability preservative surface finish. The results revealed that, the addition of KGC was beneficial in improving the total thickness of interfacial intermetallic compound (IMC) layer. At higher isothermal ageing of 150 °C and 1000 h, the IMC layer in SAC305-KGC composite solder was towards a planar-type morphology. Moreover, the growth of total interfacial IMC layer and Cu3Sn layer during isothermal ageing was found to be controlled by bulk diffusion and grain-boundary process, respectively. The activation energy possessed by SAC305-KGC composite solder for total interfacial IMC layer and Cu3Sn IMC was 74 kJ/mol and 104 kJ/mol, respectively. Based on a lap shear test, the shear strength of SAC305-KGC composite solder exhibited higher shear strength than non-reinforced SAC305 solder. Meanwhile, the solder joints failure mode after shear testing was a combination of brittle and ductile modes at higher ageing temperature and time for SAC305-KGC composite solder.
11 September 2019 in Journal of Electronic Materials
The effect of bismuth (Bi) micro-alloying additions on wettability and mechanical properties of Sn-0.7Cu lead-free solder were explored. This paper also investigates the influences of various Bi percentages on the suppression of intermetallic compound formation. Scanning electron microscope (SEM) was used to observe the microstructure evolution of solder joint including the thickness of interfacial intermetallic layers. Overall, with the addition of Bi to Sn-0.7Cu solder, the size of primary Cu6Sn5 become smaller and suppresses the thickness of interfacial intermetallic compound between solder and the Cu substrate. Microhardness value and wetting properties also increased with Bi addition which resulted in smaller size of β-Sn and Cu6Sn5.