This study evaluated the effect of UV absorbers on the dimensional accuracy of zirconia specimens fabricated by additive manufacturing using a digital light process. Zirconia suspension for additive manufacturing was prepared by setting the volume fractions (0, 0.005, 0.05, and 0.1%) of various UV absorbers. The effect of UV absorber content was evaluated through curing thickness, geometric overgrowth model design, linear deviation, and microstructure evaluation before and after sintering. Statistical analysis was performed by Kruskal–Wallis H and post-tested by the Bonferroni correction method. There was no significant difference in the cure depth according to the presence or absence of the UV absorber, the difference in geometric overgrowth was from 2.1 to 12.5%, and the overgrowth significantly decreased as the amount of added UV absorber increased. This result may contribute to improved precision of 3D multilayer ceramic products.
To prepare a photocurable ceramic suspension for use in commercialized additive manufacturing equipment, the effects of the rheological properties of zirconia particles added to a binder, and the presence or absence of a silane coupling agent on the particles was evaluated. To this end, three experimental groups (ZSs, ZMs, ZLs) and three control groups (ZS, ZM, ZL) were designed depending on the size of the underlying zirconia particles. The test-group zirconia suspensions were prepared through silanization, which was not applied to the control-group suspensions. Depending on the particle size, viscosity differences between the test and control groups were 16,842, 18,623, and 12,303 mPa·s, respectively. Compared to the other groups, the viscosity of the ZLs group suspension decreased by 70.98–88.04%. This confirmed that the viscosity of the suspensions was affected by the particle size and the presence of silane coating. The dispersion stability of the zirconia suspensions was evaluated over 20 days. A sedimentation test confirmed that the sedimentation rate of the ZLs group was slower than those of the other groups. This study aimed to optimize the suspension manufacturing method to effectively be utilized in further commercializing zirconia three-dimensional (3D) printing and could also help to develop various medical applications.
Traumatic tendon injuries are among the most common types of injuries, often characterized by insufficient and slow recovery. The current study aims to evaluate the regenerative capacity of a tissue-engineered tendon graft in a rabbit gastrocnemius tendon defect. This graft comprises gap-electrospun collagen-coated parallel polycaprolactone (PCL) fibers seeded with adipose-derived stem cells (ADSCs), which promoted to adopt a tenogenic phenotype using a tenocyte-imprinted substrate for the first time. Scanning electron microscopy (SEM) images confirmed the parallel structure and successful cell attachment to the scaffold. Sirius red staining, high-performance X-ray photoelectron spectroscopy, and water contact angle showed that collagen successfully coated and changed the surface hydrophilicity of the scaffold. Imprinted substrates showed tenocyte patterns in SEM images. In an in vitro evaluation, ICC and real-time polymerase chain reaction confirmed that the stem cells acquired tenogenic traits. In addition, histopathology scoring outcomes showed significant improvement in the Pattern group and an almost 2.58 times increase in the total score average compared to the control group. In vitro and in vivo therapy results show that differentiated ADSCs seeded on the collagen-coated PCL scaffold for tendon repair have astounding therapeutic potential.
Although the clinical need for bioengineered blood vessels is growing, options for vascular conduits are currently limited. The aim of this study is to develop a novel scaffold fabrication method for use as a small-diameter vascular graft and to evaluate its biocompatibility, cell attachment, and mechanical properties. This scaffold consists of a tubular polycaprolactone parallel nanofiber section (a seamless tube of fibers aligned along the long axis) reinforced with 4-axis 3D printed spiral polycaprolactone. The final structure was coated with collagen and cultured with various cells. High-resolution field emission-scanning electron microscopy images confirm the successful fabrication of seamless parallel fibrous tubes (as small as 300 µm) and fusion of the fibers to the spiral reinforcement. Biocompatibility assays on the scaffold indicate no cell toxicity, and the parallel fibers successfully oriented the cells cultured inside the tube, thereby mimicking their natural orientation in vascular tissue. The spiral reinforcement was successfully attached to the inner tube, which significantly improved the tube's mechanical strength compared to the non-reinforced groups. These results suggest that this new fabrication method of polycaprolactone/collagen parallel tubular nanofibers reinforced by using 4-axis 3D printing techniques could play a promising role in future bioengineered vascular tissues or other tubular tissues.