Gold nanoparticles on the surface of cerium(IV) oxide were obtained by photochemical reduction of HAuCl4 in water–alcohol solutions. The spectral characteristics of the resultant nanocomposites, their phase composition and morphology, and the kinetics of the gold particles formation were examined depending on the nature of the monohydric alcohol and on the morphology of the cerium(IV) oxide particles. The catalytic activity of cerium(IV) oxide before and after modification with gold nanoparticles in the reactions of photodegradation of methyl orange and phenol was studied. It was shown that the CeO2 particles modified with gold nanoparticles upon irradiation with UV light have the highest photocatalytic activity.
The article discusses the possibilities of fine composition variation of polycrystalline PZT films at the morphotropic phase boundary. The composition of thin films prepared by RF magnetron sputtering of a ceramic target of stoichiometric composition PbZr0.54Ti0.46O3 was varied by changing the distance from the target to the substrate in the range of 30–70 mm. This made it possible to change the composition by ~1.5%. The study focused on the dielectric properties of the formed self-polarized films. The study found that the resistance to external electric fields depends on the conditions of film preparation.
The article discusses electron energy loss of bulk and surface plasmons in solid polycrystalline Mg films. The experimental study of the electrons’ characteristic energy loss is conducted and its results are compared in a wide range of electron incidence angles on the sample (0°–89°), dispersion angles (5°–165°) and electron energies (100–600 eV). Electron wave refraction at the vacuum–solid state interface is considered as one of the factors determining the intensity of surface plasmons.